# What Are Corrosion Resistant Alloys (CRAs)?

> A corrosion resistant alloy is chosen by the medium, not the datasheet. How the nickel CRA families split — Ni-Cr-Mo, Ni-Mo, Ni-Cr, Ni-Cu — and how to shortlist one.

A corrosion resistant alloy is not a grade that resists everything. It is a grade matched to one set of conditions — a medium, a concentration, an aeration state and a temperature — and the families differ mostly in which of those conditions they were built for. That is why two alloys with similar nickel content can behave completely differently in the same vessel.

## Key takeaways

- Corrosion resistant alloys are selected by **medium first**, temperature second. The reverse order produces expensive failures.
- The nickel CRA families split by chemistry: **Ni-Cr-Mo** for mixed oxidising and reducing service, **Ni-Mo** for reducing acids, **Ni-Cr** and **Ni-Cr-Mo-Nb** for oxidation at temperature, **Ni-Cu** for seawater and hydrofluoric acid.
- **A higher temperature ceiling is not better corrosion resistance.** Inconel 600 and Incoloy 800HT carry the highest service ceilings in a typical CRA stock list, and neither is the answer for an aggressive acid.
- Chromium helps in oxidising conditions and can hurt in strongly reducing ones, which is why the Ni-Mo grades carry no chromium at all.
- The form matters after the chemistry: plate, sheet, bar, wire, forging and tube availability decide what can actually be built.

## What a corrosion resistant alloy actually is

Any alloy chosen primarily for its resistance to a corrosive environment qualifies, which makes the term broader than most buyers expect: it covers stainless steels, nickel alloys, titanium and several others. In practice, when a specification says "CRA" it means the alloy is being selected against a corrosion duty rather than a strength or weight duty, and the corrosion engineer owns the decision.

The reason nickel alloys dominate the high end of that list is metallurgical rather than commercial. Nickel holds a large amount of alloying element in solid solution, so molybdenum and chromium can be added together without the structure becoming unstable. That combination is what lets one grade handle both oxidising and reducing conditions — a balance stainless steels cannot reach.

## The four chemistry families, and what each is for

**Ni-Cr-Mo: mixed oxidising and reducing service.** [Hastelloy C-276](/alloys/hastelloy-c-276/), [C22](/alloys/hastelloy-c22/) and [C-4](/alloys/hastelloy-c-4/) are the general-purpose CRA family. C-276 is the default when the medium is not fully characterised, because molybdenum covers reducing attack while chromium covers oxidising attack. C22 pushes further on oxidising media, and C-4 targets chemical equipment where intergranular precipitation during service and welding is the concern. The grade data lists service to 400 °C for C-276 and 600 °C for C22 and C-4.

**Ni-Mo: reducing acids.** [Hastelloy B-2](/alloys/hastelloy-b-2/) and [B-3](/alloys/hastelloy-b-3/) (N10675) are the deliberate exception to the chromium rule. They are formulated for reducing acid service, where a chromium-bearing alloy is attacked rather than protected. B-3 is the third-generation Ni-Mo grade, with thermal stability and fabricability improved over B-2. Both are listed to 650 °C.

**Ni-Cr and Ni-Cr-Mo-Nb: oxidation at temperature.** [Inconel 600](/alloys/inconel-600/) is a Ni-Cr alloy listed to 1095 °C, [Inconel 625](/alloys/inconel-625/) adds molybdenum and niobium for corrosion resistance plus strength to 980 °C, and [Incoloy 800HT](/alloys/incoloy-800ht/) is the Ni-Fe-Cr grade with high-temperature ductility to 1100 °C. These are the grades that appear when the duty is scale and oxidation rather than immersion.

**Ni-Cu: seawater and hydrofluoric acid.** [Monel 400](/alloys/monel-400/) is the outlier in nickel terms — a nickel-copper alloy listed to 540 °C, chosen for marine service and hydrofluoric acid where the nickel-rich chemistries are either unnecessary or attacked.

## Choosing by medium, not by datasheet

The practical shortlist comes from four questions, asked in this order:

1. **Which medium?** Oxidising acids, reducing acids, chlorides and seawater, or high-temperature oxidation all point at different families.
2. **What concentration, and is it aerated?** Aeration changes the answer as much as concentration does, and it is the detail most often missing from a purchase enquiry.
3. **What temperature?** This sets both the corrosion rate and the mechanical allowance, and it can eliminate a grade that looked ideal on paper.
4. **What form?** Plate, sheet, strip, bar, forging, wire and tube are not available in every grade at every size, so availability sometimes reshapes the shortlist late.

Only after those four does the standard, the tolerance and the certificate matter — and those are properties of the order, not of the alloy family.

## Where CRAs are used in practice

The applications cluster in chemical processing, flue-gas desulfurization and pollution control, pulp and paper bleaching, sour gas service, marine and offshore hardware, and high-temperature furnace internals. The common thread is that a cheaper material failed first: the CRA is specified after a corrosion allowance became unworkable, not as a first choice.

That history also explains why the grade list is short. Each family exists because a specific failure mode — chloride stress corrosion cracking, pitting under deposits, reducing-acid attack — had no cheaper answer.

## Shortlisting from a [nine-grade stock list](/alloys/)

RAS Thermal stocks nine grades across those four families, each with its UNS number, service ceiling, available forms and standards. The [selection guide](/hub/corrosion-resistant-alloys/) groups them by medium, which is the order in which the decision is actually made: mixed oxidising and reducing service (C-276, C22, C-4), reducing acids (B-2, B-3), seawater and hydrofluoric acid (Monel 400), and oxidation at temperature (600, 625, 800HT).

The next step after the shortlist is the grade page, and after that the certificate. If the medium is genuinely not characterised yet, say so in the enquiry — that single sentence usually removes two grades from the list and one round of testing from the schedule.