Ask a superalloy density and weight question about Hastelloy C-276 (N10276) and the answer lives in the verified reference data Hastelloy C-276 is built to. This is the specification guide to superalloy density and weight on Hastelloy C-276, drawn from RAS Thermal’s superalloy documentation.
Hastelloy C-276 (N10276) is a Hastelloy alloy rated to 400 °C, stocked for Chemical reactor internals.
The verified composition band for Hastelloy C-276 (N10276) is Mo 15.0-17.0%, Cr 14.5-16.5%, Fe 4.0-7.0%, W 3.0-4.5%; that band is what the mill certificate is checked against, element by element.
What Superalloy Density and Weight means for Hastelloy C-276
Hastelloy C-276 (N10276) on superalloy density and weight: density 8.89 g/cm³, verified ceiling 400 °C. The deciding facts are temperature, media and form, and they land on chemical reactor internals, FGD scrubbers and sour-gas piping where pitting and stress-corrosion cracking are the enemy.
| Property | Hastelloy C-276 |
|---|---|
| Grade | Hastelloy C-276 (N10276) |
| Density | 8.89 g/cm³ |
| Max service temp | 400 °C |
| Best duty | Chemical reactor internals, FGD scrubbers and sour-gas piping where pitting and stress-corrosion cracking are the enemy |
| Available forms | Forging, Wire, Plate, Sheet, Strip, Bar, Tube |
| Standards | ASTM B575, ASTM B574, ASTM B564, UNS N10276 |
Specification signals
One verified figure, 8.89 g/cm³, sits beneath the whole weight discussion for Hastelloy C-276. In practice the applications list confirms the fit: Hastelloy C-276 is specified for chemical reactor internals and flue-gas desulfurization scrubbers, not as a universal filler.
- One Hastelloy C-276 datasheet callout does most of the work on this page: Good weldability without post-weld heat treatment. A purchasing audit on the Hastelloy C-276 order checks that line first.
In practice
Refractory content is what moves the nickel line up and down the density scale. Mass budgets for chemical reactor internals, FGD scrubbers and sour-gas piping where pitting and stress-corrosion cracking are the enemy start here.
How to select the right option for your process
Five checks, in order. Each one keeps the component inside its specification:
- Step 1: Confirm the maximum service temperature. Fix the peak continuous service temperature the component will see. It decides whether a precipitation-hardened grade such as Inconel 718 (rated 650 °C) or an oxidation-resistant solid-solution grade such as Hastelloy X (rated 1100 °C) is even in the running.
- Step 2: Match the environment and alloy family. Identify the corroding or oxidizing media (chlorides, acids, seawater, combustion gas) and match the family: Ni-Cr-Mo for wet corrosion, Ni-Cu for seawater and hydrofluoric acid, cobalt-base for wear and biocompatibility, precision grades for controlled physical properties.
- Step 3: Choose the product form. Select the semi-finished form: bar and rod (Ø6-350 mm), plate and sheet (0.5-80 mm), strip (0.05-3.0 mm), pipe and tube (OD 6-219 mm), wire (Ø0.10-12.0 mm) or a forged ring, disc or shaft from 5 kg to 3,000 kg.
- Step 4: Set the dimensions and tolerances. State the finished dimensions, condition (hot rolled, cold drawn, solution annealed, spring temper) and surface finish against the form’s stock range, so the mill certificate matches the drawing.
- Step 5: State the standard and certificate. Declare the governing ASTM / AMS / GB/T standard and the certification level: EN 10204 3.1 with heat-specific chemistry, or 3.2 third-party witnessed. The grade is proven by the mill test certificate, not assumed.
Frequently Asked Questions (FAQ)
How does superalloy density and weight resolve for Hastelloy C-276?
Density does the arithmetic quietly, and for Hastelloy C-276 the arithmetic begins at 8.89 g/cm³. Multiply 8.89 g/cm³ by the section volume and the quote’s mass line stops being a surprise.
What is Hastelloy C-276 best used for?
Hastelloy C-276 is stocked for chemical reactor internals, FGD scrubbers and sour-gas piping where pitting and stress-corrosion cracking are the enemy; the documented edge is that the general-purpose Ni-Cr-Mo corrosion grade for aggressive wet service, weldable without post-weld heat treatment.
What forms is Hastelloy C-276 available in?
Stocked forms: Forging, Wire, Plate, Sheet, Strip, Bar, Tube.
What standards does Hastelloy C-276 meet?
Every Hastelloy C-276 order cites its governing standard (ASTM B575, ASTM B574, ASTM B564, UNS N10276) and arrives with an EN 10204 3.1 certificate proving the heat.
When does Hastelloy C-276 stop being the right choice?
Hastelloy C-276 stops being right above 400 °C, or in media its family was not built for.