Ask a superalloy density and weight question about Nickel 200 (N02200) and the answer lives in the verified reference data Nickel 200 is built to. This is the specification guide to superalloy density and weight on Nickel 200, drawn from RAS Thermal’s superalloy documentation.
Nickel 200 (N02200): Commercially pure wrought nickel for caustic soda, synthetic fiber and electrical applications..
For reference, the verified chemistry bands include Monel K-500 at Ni 63.0-70.0% and Cu 27.0-33.0%, plus Nickel 200 at 99.6% minimum nickel. The certificates cite the same bands.
What Superalloy Density and Weight means for Nickel 200
For Nickel 200 (N02200), superalloy density and weight comes down to the documented envelope: 8.89 g/cm³, 315 °C ceiling, and a duty best described as caustic soda evaporator tubes, spinnerets and electrical terminals.
| Property | Nickel 200 |
|---|---|
| Grade | Nickel 200 (N02200) · GB N6 |
| Density | 8.89 g/cm³ |
| Max service temp | 315 °C |
| Best duty | Caustic soda evaporator tubes, spinnerets and electrical terminals |
| Available forms | Forging, Wire, Flange, Bar & Rod, Plate & Sheet, Strip, Pipe & Tube |
| Standards | ASTM B160, ASTM B161, ASTM B162, ASME SB-160 |
Specification signals
The mass conversation for Nickel 200 opens and closes with 8.89 g/cm³. In practice the applications list confirms the fit: Nickel 200 is specified for caustic soda evaporator tubes and synthetic fiber spinnerets, not as a universal filler.
- One Nickel 200 datasheet callout does most of the work on this page: High electrical conductivity. A purchasing audit on the Nickel 200 order checks that line first.
In practice
Every kilogram on the cost line traces back to this multiplication. caustic soda evaporator tubes, spinnerets and electrical terminals inherits that number directly.
How to select the right option for your process
Run the list top to bottom before the enquiry goes out, that is what keeps the part inside its specification:
- Step 1: Confirm the maximum service temperature. Fix the peak continuous service temperature the component will see. It decides whether a precipitation-hardened grade such as Inconel 718 (rated 650 °C) or an oxidation-resistant solid-solution grade such as Hastelloy X (rated 1100 °C) is even in the running.
- Step 2: Match the environment and alloy family. Identify the corroding or oxidizing media (chlorides, acids, seawater, combustion gas) and match the family: Ni-Cr-Mo for wet corrosion, Ni-Cu for seawater and hydrofluoric acid, cobalt-base for wear and biocompatibility, precision grades for controlled physical properties.
- Step 3: Choose the product form. Select the semi-finished form: bar and rod (Ø6-350 mm), plate and sheet (0.5-80 mm), strip (0.05-3.0 mm), pipe and tube (OD 6-219 mm), wire (Ø0.10-12.0 mm) or a forged ring, disc or shaft from 5 kg to 3,000 kg.
- Step 4: Set the dimensions and tolerances. State the finished dimensions, condition (hot rolled, cold drawn, solution annealed, spring temper) and surface finish against the form’s stock range, so the mill certificate matches the drawing.
- Step 5: State the standard and certificate. Declare the governing ASTM / AMS / GB/T standard and the certification level: EN 10204 3.1 with heat-specific chemistry, or 3.2 third-party witnessed. The grade is proven by the mill test certificate, not assumed.
Frequently Asked Questions (FAQ)
How does superalloy density and weight resolve for Nickel 200?
Density, verified for Nickel 200: 8.89 g/cm³. On weight-budgeted hardware the density is a design input, not trivia. It scales every volume-based cost line.
What is Nickel 200 best used for?
Caustic soda evaporator tubes, spinnerets and electrical terminals. Commercially pure wrought nickel (99.6% min) for caustic alkalis and electrical duty.
What forms is Nickel 200 available in?
Stocked forms: Forging, Wire, Flange, Bar & Rod, Plate & Sheet, Strip, Pipe & Tube.
What standards does Nickel 200 meet?
Every Nickel 200 order cites its governing standard (ASTM B160, ASTM B161, ASTM B162, ASME SB-160) and arrives with an EN 10204 3.1 certificate proving the heat.
When does Nickel 200 stop being the right choice?
The ceiling is 315 °C and the family is fixed, so anything hotter or more aggressive calls for a different grade.