Inconel 718 is the same alloy under many names: UNS N07718 in the US, W.Nr 2.4668 (NiCr19Fe19Nb5Mo3) in the German/EN system, GH4169 in China, NC19FeNb in France and NCF 718 in Japan. The chemistry windows are aligned, so the grades are technically interchangeable, but only when the material also meets the specification the drawing calls out (AMS 5662 for bar, AMS 5596 for sheet and plate, ASTM B637 for bar and forgings). An “equivalent grade” is a chemistry statement, the acceptance document is the standard and the certificate.
Inconel 718 equivalent grades at a glance
| System | Designation | Relevant standard |
|---|---|---|
| USA (UNS) | N07718 | ASTM B637 · ASTM B670 |
| USA (aerospace bar) | Alloy 718 | AMS 5662 / 5663 / 5664 |
| USA (aerospace sheet & plate) | Alloy 718 | AMS 5596 / 5597 |
| Germany / EN | W.Nr. 2.4668 · NiCr19Fe19Nb5Mo3 | DIN 17744 / 17753 · EN 10095 |
| China | GH4169 (GH169), ISC H41690 | GB/T 14992 · GJB 2611A |
| France | NC19FeNb | AFNOR |
| UK | NA 51 · HR 202 | BS |
| Japan | NCF 718 | JIS G4901 |
| ISO | NW7718 · NiCr19Fe19Nb5Mo3 | ISO 15156 (NACE MR0175) for sour service |
These are the designations that appear on mill certificates and mill test reports, the grade chemistry behind them is the same γ″-strengthened Ni-Cr-Fe system.
Which specification governs which product form
This is where “equivalent” stops being interchangeable in practice. Each form has its own governing document:
| Form | ASTM | AMS |
|---|---|---|
| Bar, forging, rings | ASTM B637 | AMS 5662 / 5663 / 5664 |
| Sheet, strip, plate | ASTM B670 | AMS 5596 / 5597 |
The AMS and ASTM documents both fix chemistry, but the AMS aerospace specifications layer on tighter trace-element limits, controlled melt practice (VIM + VAR for flight-critical parts) and rotating-quality inspection. A heat that passes a standard GB/T chemistry may still fail an aerospace cleanliness requirement, which is why an “equivalent grade” is not an “equivalent acceptance”.
Why the chemistry matches, and why certification still differs
The strengthening mechanism is the coherent γ″ (Ni₃Nb) precipitate, which is why the niobium window (4.75-5.50 %) is the tightest line in the specification: too little Nb and the strength target is missed, too much and Laves or δ phase forms and hurts ductility. The nickel matrix is 50.0-55.0 % with 17.0-21.0 % Cr, 2.80-3.30 % Mo, 0.65-1.15 % Ti and 0.20-0.80 % Al: identical across GH4169 (GB/T 14992 / GJB 2611A) and AMS 5662, element by element. What differs between an industrial-grade GH4169 and a flight-critical alloy 718 is not chemistry but melt practice and documentation: VIM + VAR refining, ultrasonic inspection and a heat-traceable EN 10204 certificate.
Mechanical equivalence
Condition, not country of origin, sets the numbers. The verified Inconel 718 design data on this site is:
| Condition | UTS | Yield (0.2 %) | Elongation | Hardness |
|---|---|---|---|---|
| Room temperature | 1275 MPa | 1035 MPa | 12% | 38 HRC |
| 540 °C | 1105 MPa | 965 MPa | 14% | n/a |
| 650 °C | 860 MPa | 795 MPa | 18% | n/a |
Supplementary, from the AMS 5662 basis: at 650 °C the yield strength floor is ≥850 MPa, the tensile floor ≥1000 MPa, and the stress-rupture life ≥100 h at 650 °C / 690 MPa. A properly processed GH4169 bar reaches the same floor as an AMS 5663 bar of the same condition.
How to specify an equivalent grade
Write the requirement in three layers so the certificate can be checked against it: (1) the grade and UNS, Inconel 718 / Alloy 718, UNS N07718; (2) the governing standard for the form, AMS 5662 for bar and forgings, AMS 5596 for sheet, strip and plate, or ASTM B637 / B670 for the industrial equivalent; (3) the condition and certificate, solution + aged (double aged) with EN 10204 3.1 heat chemistry, or 3.2 third-party witnessed for aerospace. If a national designation such as GH4169 is offered as an equivalent, require the chemistry to be reported against the AMS or ASTM window. That is what makes the substitution defensible.
How to select the right option for your process
Five checks, in order. Each one keeps the component inside its specification:
- Step 1: Confirm the maximum service temperature. Fix the peak continuous service temperature the component will see. It decides whether a precipitation-hardened grade such as Inconel 718 (rated 650 °C) or an oxidation-resistant solid-solution grade such as Hastelloy X (rated 1100 °C) is even in the running.
- Step 2: Match the environment and alloy family. Identify the corroding or oxidizing media (chlorides, acids, seawater, combustion gas) and match the family: Ni-Cr-Mo for wet corrosion, Ni-Cu for seawater and hydrofluoric acid, cobalt-base for wear and biocompatibility, precision grades for controlled physical properties.
- Step 3: Choose the product form. Select the semi-finished form: bar and rod (Ø6-350 mm), plate and sheet (0.5-80 mm), strip (0.05-3.0 mm), pipe and tube (OD 6-219 mm), wire (Ø0.10-12.0 mm) or a forged ring, disc or shaft from 5 kg to 3,000 kg.
- Step 4: Set the dimensions and tolerances. State the finished dimensions, condition (hot rolled, cold drawn, solution annealed, spring temper) and surface finish against the form’s stock range, so the mill certificate matches the drawing.
- Step 5: State the standard and certificate. Declare the governing ASTM / AMS / GB/T standard and the certification level: EN 10204 3.1 with heat-specific chemistry, or 3.2 third-party witnessed. The grade is proven by the mill test certificate, not assumed.
Frequently Asked Questions (FAQ)
Is GH4169 the same as Inconel 718?
Yes, GH4169 (also written GH169, ISC H41690) is the Chinese designation for the same Ni-Cr-Fe γ″-strengthened alloy as UNS N07718 / Inconel 718, with chemistry aligned element by element under GB/T 14992 and GJB 2611A. It is interchangeable where the material also meets the AMS or ASTM specification the drawing calls out.
What is W.Nr 2.4668?
It is the German/EN Werkstoff number for Inconel 718, also written NiCr19Fe19Nb5Mo3, defined under DIN 17744 / 17753 and EN 10095. It is the same alloy as UNS N07718.
Which AMS number covers 718 plate rather than bar?
AMS 5596 (and 5597) cover 718 sheet, strip and plate; AMS 5662 / 5663 / 5664 cover bar, forgings and rings. The form decides which AMS document applies.
Are GH4169 and Inconel 718 always interchangeable?
Chemically yes; in acceptance, only if the offered material meets the standard the design specifies. Aerospace and gas-turbine parts usually require VIM + VAR melt practice and AMS 5662/5663 documentation, which commercial single-melt GH4169 does not automatically provide.