What MP35N (R30035) can and cannot do on superalloy hardness (hrc / hrb) is fixed by the verified envelope below. Datasheet facts on MP35N, and the decision they drive for superalloy hardness (hrc / hrb). Nothing else.
MP35N (R30035) is a Cobalt-Based alloy rated to 425 °C, stocked for Medical implants and guidewires.
For reference, the precision-alloy anchors are 4J36 (Invar 36) at a near-zero expansion coefficient of about 1.3 × 10⁻⁶/°C from cryogenic to 230 °C, and 1J22 at the highest saturation induction of any commercial soft magnetic material, 2.4 T.
What Superalloy Hardness (HRC / HRB) means for MP35N
For MP35N (R30035), superalloy hardness (hrc / hrb) comes down to the documented envelope: 8.43 g/cm³, 425 °C ceiling, and a duty best described as medical implants, aerospace fasteners and high-performance springs.
| Property | MP35N |
|---|---|
| Grade | MP35N (R30035) |
| Density | 8.43 g/cm³ |
| Max service temp | 425 °C |
| Best duty | Medical implants, aerospace fasteners and high-performance springs |
| Available forms | Forging, Wire, Spring Wire, Bar & Rod, Strip |
| Standards | ASTM F562, AMS 5844, AMS 5845, ISO 5832-6 |
Specification signals
Treatment in, band out. The documented applications tell the same story (medical implants and guidewires, aerospace fasteners), and a duty outside that list deserves a second look before MP35N goes on the order.
- One MP35N datasheet callout does most of the work on this page: Non-magnetic (MRI compatible). A purchasing audit on the MP35N order checks that line first.
In practice
Grade comparisons that skip the condition step compare nothing, since the treatment sets most of the band. The hardness class and medical implants, aerospace fasteners and high-performance springs go together on the purchase order.
How to select the right option for your process
Work through these checks in order so the component stays inside its specification:
- Step 1: Confirm the maximum service temperature. Fix the peak continuous service temperature the component will see. It decides whether a precipitation-hardened grade such as Inconel 718 (rated 650 °C) or an oxidation-resistant solid-solution grade such as Hastelloy X (rated 1100 °C) is even in the running.
- Step 2: Match the environment and alloy family. Identify the corroding or oxidizing media (chlorides, acids, seawater, combustion gas) and match the family: Ni-Cr-Mo for wet corrosion, Ni-Cu for seawater and hydrofluoric acid, cobalt-base for wear and biocompatibility, precision grades for controlled physical properties.
- Step 3: Choose the product form. Select the semi-finished form: bar and rod (Ø6-350 mm), plate and sheet (0.5-80 mm), strip (0.05-3.0 mm), pipe and tube (OD 6-219 mm), wire (Ø0.10-12.0 mm) or a forged ring, disc or shaft from 5 kg to 3,000 kg.
- Step 4: Set the dimensions and tolerances. State the finished dimensions, condition (hot rolled, cold drawn, solution annealed, spring temper) and surface finish against the form’s stock range, so the mill certificate matches the drawing.
- Step 5: State the standard and certificate. Declare the governing ASTM / AMS / GB/T standard and the certification level: EN 10204 3.1 with heat-specific chemistry, or 3.2 third-party witnessed. The grade is proven by the mill test certificate, not assumed.
Frequently Asked Questions (FAQ)
How does superalloy hardness (hrc / hrb) resolve for MP35N?
Ask about hardness for MP35N and the honest answer begins with annealed, solution-treated or age-hardened. The EN 10204 3.1 certificate is where the actual hardness of your heat appears.
What is MP35N best used for?
MP35N is stocked for medical implants, aerospace fasteners and high-performance springs; the documented edge is that a Co-Ni-Cr-Mo grade with ultra-high tensile strength (over 1800 MPa achievable), non-magnetic and MRI compatible.
What forms is MP35N available in?
MP35N ships as Forging, Wire, Spring Wire, Bar & Rod, Strip, within the stock range of each form.
What standards does MP35N meet?
Every MP35N order cites its governing standard (ASTM F562, AMS 5844, AMS 5845, ISO 5832-6) and arrives with an EN 10204 3.1 certificate proving the heat.
When does MP35N stop being the right choice?
MP35N stops being right above 425 °C, or in media its family was not built for.