Superalloy Hardness (HRC / HRB), applied to Waspaloy (N07001): verified numbers first, then the reasoning a specifier applies to Waspaloy. A RAS Thermal reference page on superalloy hardness (hrc / hrb).

Waspaloy is a precipitation-hardenable nickel-chromium-cobalt superalloy with exceptional creep-rupture strength at elevated temperatures.

As a chemistry anchor from the verified composition tables, Inconel 718 spans Ni 50.0-55.0%, Cr 17.0-21.0%, Mo 2.80-3.30% and Nb 4.75-5.50%, and Hastelloy C-276 spans Mo 15.0-17.0%, Cr 14.5-16.5%, Fe 4.0-7.0% and W 3.0-4.5%.

What Superalloy Hardness (HRC / HRB) means for Waspaloy

Waspaloy (N07001) on superalloy hardness (hrc / hrb): density 8.22 g/cm³, verified ceiling 870 °C. The deciding facts are temperature, media and form, and they land on turbine discs, rings, shafts and high-temperature fasteners.

PropertyWaspaloy
GradeWaspaloy (N07001) · GB GH4738
Density8.22 g/cm³
Max service temp870 °C
Best dutyTurbine discs, rings, shafts and high-temperature fasteners
Available formsForging, Wire, Flange, Bar & Rod, Plate & Sheet, Strip
StandardsAMS 5708, AMS 5709, AMS 5544, ASTM B637

Specification signals

Waspaloy is supplied to the hardness band its condition implies, and the certificate states the value. The documented applications tell the same story (turbine discs and rings, compressor shafts), and a duty outside that list deserves a second look before Waspaloy goes on the order.

  • The feature that separates Waspaloy from its nearest neighbours is specific: Precipitation-hardenable for turbine applications. Hold the Waspaloy certificate to proving it, not asserting it.

In practice

Purchase orders that name the treatment give the inspector a concrete band to audit when the certificate arrives. One line settles it.

How to select the right option for your process

Work through these checks in order so the component stays inside its specification:

  1. Step 1: Confirm the maximum service temperature. Fix the peak continuous service temperature the component will see. It decides whether a precipitation-hardened grade such as Inconel 718 (rated 650 °C) or an oxidation-resistant solid-solution grade such as Hastelloy X (rated 1100 °C) is even in the running.
  2. Step 2: Match the environment and alloy family. Identify the corroding or oxidizing media (chlorides, acids, seawater, combustion gas) and match the family: Ni-Cr-Mo for wet corrosion, Ni-Cu for seawater and hydrofluoric acid, cobalt-base for wear and biocompatibility, precision grades for controlled physical properties.
  3. Step 3: Choose the product form. Select the semi-finished form: bar and rod (Ø6-350 mm), plate and sheet (0.5-80 mm), strip (0.05-3.0 mm), pipe and tube (OD 6-219 mm), wire (Ø0.10-12.0 mm) or a forged ring, disc or shaft from 5 kg to 3,000 kg.
  4. Step 4: Set the dimensions and tolerances. State the finished dimensions, condition (hot rolled, cold drawn, solution annealed, spring temper) and surface finish against the form’s stock range, so the mill certificate matches the drawing.
  5. Step 5: State the standard and certificate. Declare the governing ASTM / AMS / GB/T standard and the certification level: EN 10204 3.1 with heat-specific chemistry, or 3.2 third-party witnessed. The grade is proven by the mill test certificate, not assumed.

Frequently Asked Questions (FAQ)

How does superalloy hardness (hrc / hrb) resolve for Waspaloy?

Waspaloy is supplied to the hardness band its condition implies, and the certificate states the value. Two heats of Waspaloy in different treatments are not comparable on hardness until the condition label sits beside both readings.

What is Waspaloy best used for?

Turbine discs, rings, shafts and high-temperature fasteners. A Ni-Cr-Co age-hardenable grade with creep-rupture strength across 650 to 870 °C.

What forms is Waspaloy available in?

Stocked forms: Forging, Wire, Flange, Bar & Rod, Plate & Sheet, Strip.

What standards does Waspaloy meet?

Waspaloy ships against AMS 5708, AMS 5709, AMS 5544, ASTM B637 as specified, with an EN 10204 3.1 certificate that actually proves the grade.

When does Waspaloy stop being the right choice?

The ceiling is 870 °C and the family is fixed, so anything hotter or more aggressive calls for a different grade.