1J22 is the answer to one question: how much magnetic flux can you force through the smallest possible cross-section? Its verified saturation induction of 2.4 T is the highest of any commercial soft magnetic material, which is why weight- and volume-critical magnetic hardware, aerospace solenoid armatures, magnetic bearing pole pieces, high-flux generator rotors, is built on it. The trade is cost and brittleness, and the design question is whether your flux density budget actually needs 2.4 T.

1J22 (HiperCo 50 equivalent) is an iron-cobalt-vanadium soft magnetic alloy offering the highest saturation magnetic induction (2.4 T) of any commercial magnetic material.

What 2.4 T saturation buys you

A magnetic circuit sized on 1J22 can carry more flux per square millimetre than one sized on any other soft magnetic grade, because the saturation induction is the ceiling the circuit can never push past, and 1J22’s ceiling is the highest verified figure in the range at 2.4 T. The second number that matters is the Curie temperature: 940 °C, far above the 450 °C service ceiling, so the alloy never loses its ferromagnetism inside its own working envelope. For aircraft power generation and precision electromagnetic actuators, that combination, flux ceiling first, Curie margin second, is why the grade exists.

Property1J22 (verified)
Saturation induction2.4 T (highest of any soft magnetic material)
Curie temperature940 °C
Max service temperature450 °C
Density8.2 g/cm³
Governing standardsGB/T 14986, ASTM A801, AMS 7717 equivalent
Stock formsWire, Strip, Plate & Sheet, Bar & Rod

Specification signals

The listed applications all spend the flux ceiling rather than the Curie margin: aerospace solenoid armatures and magnetic bearing pole pieces push maximum flux through minimum section, high-flux generator rotors and aircraft power generation spend it where every gram of iron removed is thrust gained, and precision electromagnetic actuators use the same density-versus-flux trade at instrument scale. Strip and plate carry the lamination and pole-piece duty, and wire and bar the rest.

  • Weight-critical magnetics: solenoid armatures, pole pieces and magnetic bearings sized on the 2.4 T ceiling
  • Power generation: high-flux generator rotors and aircraft power generation where flux per gram decides
  • Actuators: precision electromagnetic actuators needing the same flux in less volume

Where 1J22 stops being the answer

If the magnetic circuit saturates below 2.4 T anyway, a cheaper Fe-Si or Fe-Ni grade does the job and 1J22 is money spent for nothing. If the duty is permeability rather than flux ceiling, shielding, instrument transformers, 1J50 is the pick. 1J22 is for the circuits that actually run near saturation: cite GB/T 14986 or ASTM A801, and let the certificate prove the chemistry.

How to select the right option for your process

Work through these checks in order so the component stays inside its specification:

  1. Step 1: Confirm the maximum service temperature. Fix the peak continuous service temperature the component will see. It decides whether a precipitation-hardened grade such as Inconel 718 (rated 650 °C) or an oxidation-resistant solid-solution grade such as Hastelloy X (rated 1100 °C) is even in the running.
  2. Step 2: Match the environment and alloy family. Identify the corroding or oxidizing media (chlorides, acids, seawater, combustion gas) and match the family: Ni-Cr-Mo for wet corrosion, Ni-Cu for seawater and hydrofluoric acid, cobalt-base for wear and biocompatibility, precision grades for controlled physical properties.
  3. Step 3: Choose the product form. Select the semi-finished form: bar and rod (Ø6-350 mm), plate and sheet (0.5-80 mm), strip (0.05-3.0 mm), pipe and tube (OD 6-219 mm), wire (Ø0.10-12.0 mm) or a forged ring, disc or shaft from 5 kg to 3,000 kg.
  4. Step 4: Set the dimensions and tolerances. State the finished dimensions, condition (hot rolled, cold drawn, solution annealed, spring temper) and surface finish against the form’s stock range, so the mill certificate matches the drawing.
  5. Step 5: State the standard and certificate. Declare the governing ASTM / AMS / GB/T standard and the certification level: EN 10204 3.1 with heat-specific chemistry, or 3.2 third-party witnessed. The grade is proven by the mill test certificate, not assumed.

Frequently Asked Questions (FAQ)

Why choose 1J22 over a standard electrical steel?

Saturation induction. 1J22 verifies 2.4 T, the highest of any commercial soft magnetic material, so a magnetic circuit sized on it carries more flux per cross-section than any electrical-steel design. If your circuit never approaches saturation, electrical steel is the economical answer.

How does the 940 °C Curie temperature relate to the 450 °C service rating?

The Curie temperature is where ferromagnetism is lost, and the 450 °C service ceiling is the datasheet’s verified mechanical and magnetic working envelope. The 490 °C of margin means the alloy stays ferromagnetic across its whole rated service range.

Is 1J22 the right alloy for magnetic shielding?

No. Shielding and transformer-core duty is decided by permeability, not the saturation ceiling. That is 1J50’s territory, with initial permeability above 30,000. 1J22 is specified when the circuit must run near its 2.4 T saturation limit.

Which standard governs a 1J22 purchase order?

GB/T 14986 for the Chinese precision-alloy designation, ASTM A801 internationally, with the AMS 7717 equivalent cited for aerospace work. The mill certificate must prove the grade by chemistry against the cited standard.