What Hastelloy C-276 (N10276) can and cannot do on superalloy maximum service temperature is fixed by the verified envelope below. Datasheet facts on Hastelloy C-276, and the decision they drive for superalloy maximum service temperature. Nothing else.

Hastelloy C-276 is a nickel-molybdenum-chromium alloy for aggressive wet-corrosion service.

The verified composition band for Hastelloy C-276 (N10276) is Mo 15.0-17.0%, Cr 14.5-16.5%, Fe 4.0-7.0%, W 3.0-4.5%; that band is what the mill certificate is checked against, element by element.

What Superalloy Maximum Service Temperature means for Hastelloy C-276

Start from the verified triple for Hastelloy C-276: 8.89 g/cm³ density, 400 °C ceiling. On superalloy maximum service temperature the duty decides, and the duty is chemical reactor internals, FGD scrubbers and sour-gas piping where pitting and stress-corrosion cracking are the enemy.

PropertyHastelloy C-276
GradeHastelloy C-276 (N10276)
Density8.89 g/cm³
Max service temp400 °C
Best dutyChemical reactor internals, FGD scrubbers and sour-gas piping where pitting and stress-corrosion cracking are the enemy
Available formsForging, Wire, Plate, Sheet, Strip, Bar, Tube
StandardsASTM B575, ASTM B574, ASTM B564, UNS N10276

Specification signals

At 400 °C, the certificate and the datasheet still agree, and that agreement is the whole reason the part gets specified. The documented applications tell the same story (chemical reactor internals, flue-gas desulfurization scrubbers), and a duty outside that list deserves a second look before Hastelloy C-276 goes on the order.

  • The feature that separates Hastelloy C-276 from its nearest neighbours is specific: Wide acid resistance range. Hold the Hastelloy C-276 certificate to proving it, not asserting it.

In practice

A ceiling means little without a known peak continuous temperature beside it. Run excursions above the line and the guarantee is gone, even when the average reads lower. Once the peak is fixed, the rest of the selection for chemical reactor internals, FGD scrubbers and sour-gas piping where pitting and stress-corrosion cracking are the enemy is comparison, not gamble.

How to select the right option for your process

Work through these checks in order so the component stays inside its specification:

  1. Step 1: Confirm the maximum service temperature. Fix the peak continuous service temperature the component will see. It decides whether a precipitation-hardened grade such as Inconel 718 (rated 650 °C) or an oxidation-resistant solid-solution grade such as Hastelloy X (rated 1100 °C) is even in the running.
  2. Step 2: Match the environment and alloy family. Identify the corroding or oxidizing media (chlorides, acids, seawater, combustion gas) and match the family: Ni-Cr-Mo for wet corrosion, Ni-Cu for seawater and hydrofluoric acid, cobalt-base for wear and biocompatibility, precision grades for controlled physical properties.
  3. Step 3: Choose the product form. Select the semi-finished form: bar and rod (Ø6-350 mm), plate and sheet (0.5-80 mm), strip (0.05-3.0 mm), pipe and tube (OD 6-219 mm), wire (Ø0.10-12.0 mm) or a forged ring, disc or shaft from 5 kg to 3,000 kg.
  4. Step 4: Set the dimensions and tolerances. State the finished dimensions, condition (hot rolled, cold drawn, solution annealed, spring temper) and surface finish against the form’s stock range, so the mill certificate matches the drawing.
  5. Step 5: State the standard and certificate. Declare the governing ASTM / AMS / GB/T standard and the certification level: EN 10204 3.1 with heat-specific chemistry, or 3.2 third-party witnessed. The grade is proven by the mill test certificate, not assumed.

Frequently Asked Questions (FAQ)

How does superalloy maximum service temperature resolve for Hastelloy C-276?

The verified ceiling for Hastelloy C-276 reads 400 °C. Not a rule of thumb, the datasheet figure. Peak matters more than average, because a short trip over 400 °C costs the guarantee that long steady running below it never touched.

What is Hastelloy C-276 best used for?

Chemical reactor internals, FGD scrubbers and sour-gas piping where pitting and stress-corrosion cracking are the enemy. The general-purpose Ni-Cr-Mo corrosion grade for aggressive wet service, weldable without post-weld heat treatment.

What forms is Hastelloy C-276 available in?

Hastelloy C-276 ships as Forging, Wire, Plate, Sheet, Strip, Bar, Tube, within the stock range of each form.

What standards does Hastelloy C-276 meet?

Every Hastelloy C-276 order cites its governing standard (ASTM B575, ASTM B574, ASTM B564, UNS N10276) and arrives with an EN 10204 3.1 certificate proving the heat.

When does Hastelloy C-276 stop being the right choice?

Hastelloy C-276 stops being right above 400 °C, or in media its family was not built for.