Ask a solid-solution vs precipitation-hardened superalloys question about Inconel 718 (N07718) and the answer lives in the verified reference data Inconel 718 is built to. This is the specification guide to solid-solution vs precipitation-hardened superalloys on Inconel 718, drawn from RAS Thermal’s superalloy documentation.
Inconel 718 (N07718) is a Inconel grade whose datasheet leans on one documented property: Precipitation-hardenable to 38 HRC.
The verified composition band for Inconel 718 (N07718) is Ni 50.0-55.0%, Cr 17.0-21.0%, Nb 4.75-5.50%, Mo 2.80-3.30%, Ti 0.65-1.15%, Al 0.20-0.80%; that band is what the mill certificate is checked against, element by element.
What Solid-Solution vs Precipitation-Hardened Superalloys means for Inconel 718
What fixes solid-solution vs precipitation-hardened superalloys for Inconel 718 (N07718) is the verified envelope (8.19 g/cm³, 650 °C) read against rotating hardware, high-strength fasteners and subsea wellhead components from cryogenic to 650 °C.
| Property | Inconel 718 |
|---|---|
| Grade | Inconel 718 (N07718) |
| Density | 8.19 g/cm³ |
| Max service temp | 650 °C |
| Best duty | Rotating hardware, high-strength fasteners and subsea wellhead components from cryogenic to 650 °C |
| Available forms | Forging, Wire, Spring Wire, Bar, Plate, Strip |
| Standards | AMS 5662, AMS 5663, ASTM B637, UNS N07718 |
Specification signals
Inconel 718 belongs to the age-hardenable camp. The feature list says so itself (Precipitation-hardenable to 38 HRC), and 650 °C is the range the aged condition is certified inside. In practice the applications list confirms the fit: Inconel 718 is specified for turbine discs and rings and compressor blades and fasteners, not as a universal filler.
- One Inconel 718 datasheet callout does most of the work on this page: Precipitation-hardenable to 38 HRC. A purchasing audit on the Inconel 718 order checks that line first.
In practice
Weld repair on an age-hardened part re-opens the local heat-treatment question. That constraint is the price of the strength. Mechanism set, duty set.
How to select the right option for your process
Run the list top to bottom before the enquiry goes out, that is what keeps the part inside its specification:
- Step 1: Confirm the maximum service temperature. Fix the peak continuous service temperature the component will see. It decides whether a precipitation-hardened grade such as Inconel 718 (rated 650 °C) or an oxidation-resistant solid-solution grade such as Hastelloy X (rated 1100 °C) is even in the running.
- Step 2: Match the environment and alloy family. Identify the corroding or oxidizing media (chlorides, acids, seawater, combustion gas) and match the family: Ni-Cr-Mo for wet corrosion, Ni-Cu for seawater and hydrofluoric acid, cobalt-base for wear and biocompatibility, precision grades for controlled physical properties.
- Step 3: Choose the product form. Select the semi-finished form: bar and rod (Ø6-350 mm), plate and sheet (0.5-80 mm), strip (0.05-3.0 mm), pipe and tube (OD 6-219 mm), wire (Ø0.10-12.0 mm) or a forged ring, disc or shaft from 5 kg to 3,000 kg.
- Step 4: Set the dimensions and tolerances. State the finished dimensions, condition (hot rolled, cold drawn, solution annealed, spring temper) and surface finish against the form’s stock range, so the mill certificate matches the drawing.
- Step 5: State the standard and certificate. Declare the governing ASTM / AMS / GB/T standard and the certification level: EN 10204 3.1 with heat-specific chemistry, or 3.2 third-party witnessed. The grade is proven by the mill test certificate, not assumed.
Frequently Asked Questions (FAQ)
How does solid-solution vs precipitation-hardened superalloys resolve for Inconel 718?
Strength is bought in the furnace, not on the chart, and Inconel 718 only collects at 650 °C once aging is written into the route. Repairs cost paperwork.
What is Inconel 718 best used for?
Rotating hardware, high-strength fasteners and subsea wellhead components from cryogenic to 650 °C. The precipitation-hardened workhorse for turbine discs and fasteners, age-hardened to 38 HRC with usable strength to 650 °C.
What forms is Inconel 718 available in?
Stocked forms: Forging, Wire, Spring Wire, Bar, Plate, Strip.
What standards does Inconel 718 meet?
Inconel 718 ships against AMS 5662, AMS 5663, ASTM B637, UNS N07718 as specified, with an EN 10204 3.1 certificate that actually proves the grade.
When does Inconel 718 stop being the right choice?
The ceiling is 650 °C and the family is fixed, so anything hotter or more aggressive calls for a different grade.