ASTM B168 covers nickel-chromium-iron alloy plate, sheet and strip, and three site grades cite it: Inconel 600, Inconel 601 and Inconel 690. The three form an oxidation-resistance ladder, 1095 °C, 1180 °C and 1100 °C verified ceilings respectively, and 690 adds the high-chromium stress-corrosion story that nuclear steam-generator hardware is built on.

A superalloy is an alloy engineered for sustained service at high temperature or in aggressive media, and every figure on this page traces back to a verified datasheet or governing standard.

As density anchors from the verified datasheets, Hastelloy X verifies 8.22 g/cm³ with oxidation resistance to 1100 °C, Inconel 625 verifies 8.44 g/cm³ to 980 °C, and L605 is the heaviest stocked grade at 9.13 g/cm³.

What the standard covers

The flat-product scope is the point: heat-treating fixtures, furnace liners and radiant tubes are fabricated from B168 sheet and plate, where the grade choice is a temperature-and-media decision. Inconel 600 (N06600, GB GH3600, 8.47 g/cm³) is the baseline Ni-Cr grade for heat-treating and chemical processing to 1095 °C. Inconel 601 (N06601, NS3103, 8.11 g/cm³) adds aluminum for superior oxidation resistance to 1180 °C, the top of the ladder and the pick for the hottest furnace hardware. Inconel 690 (N06690, NS3105, 8.19 g/cm³) raises chromium further for stress-corrosion-cracking resistance, which is why nuclear steam generator tubing is its verified duty.

Grades under this standard

GradeUNSGBDensityMax service tempStandout duty
Inconel 600N06600GH36008.47 g/cm³1095 °CHeat-treating, chemical processing
Inconel 601N06601NS31038.11 g/cm³1180 °CHottest furnace hardware (aluminum-added)
Inconel 690N06690NS31058.19 g/cm³1100 °CNuclear SCC resistance

How to order against it

Order B168 by UNS and form, with condition stated, the grades ship solution annealed for oxidation and corrosion duty. Bar and rod for the same three grades carry their own specification, and keep the form-standard pairing explicit so the certificate matches the drawing. EN 10204 3.1 heat chemistry is the proof.

How to select the right option for your process

Run the list top to bottom before the enquiry goes out, that is what keeps the part inside its specification:

  1. Step 1: Confirm the maximum service temperature. Fix the peak continuous service temperature the component will see. It decides whether a precipitation-hardened grade such as Inconel 718 (rated 650 °C) or an oxidation-resistant solid-solution grade such as Hastelloy X (rated 1100 °C) is even in the running.
  2. Step 2: Match the environment and alloy family. Identify the corroding or oxidizing media (chlorides, acids, seawater, combustion gas) and match the family: Ni-Cr-Mo for wet corrosion, Ni-Cu for seawater and hydrofluoric acid, cobalt-base for wear and biocompatibility, precision grades for controlled physical properties.
  3. Step 3: Choose the product form. Select the semi-finished form: bar and rod (Ø6-350 mm), plate and sheet (0.5-80 mm), strip (0.05-3.0 mm), pipe and tube (OD 6-219 mm), wire (Ø0.10-12.0 mm) or a forged ring, disc or shaft from 5 kg to 3,000 kg.
  4. Step 4: Set the dimensions and tolerances. State the finished dimensions, condition (hot rolled, cold drawn, solution annealed, spring temper) and surface finish against the form’s stock range, so the mill certificate matches the drawing.
  5. Step 5: State the standard and certificate. Declare the governing ASTM / AMS / GB/T standard and the certification level: EN 10204 3.1 with heat-specific chemistry, or 3.2 third-party witnessed. The grade is proven by the mill test certificate, not assumed.

Frequently Asked Questions (FAQ)

Which grades fall under ASTM B168?

The nickel-chromium-iron flat-product family, on this site, Inconel 600, Inconel 601 and Inconel 690 all cite B168 for plate, sheet and strip supply.

Which of the three resists oxidation best?

Inconel 601, at a verified 1180 °C ceiling, the aluminum addition lifts it above 600 (1095 °C) and 690 (1100 °C) for furnace-hardware duty.

Why is Inconel 690 the nuclear pick?

Its high-chromium chemistry gives superior stress-corrosion-cracking resistance, the verified reason nuclear steam generator tubing is specified in 690 despite siblings running hotter.