ASTM B408 covers nickel-iron-chromium alloy rod and bar, and on this site it belongs to Incoloy 800 (N08800, GB NS111): the cost-effective base grade of the 800 family, oxidation and carburization resistant to 1100 °C. Machined furnace components, flanges and fittings cut from B408 bar are the everyday face of this specification.

A superalloy is an alloy engineered for sustained service at high temperature or in aggressive media, and every figure on this page traces back to a verified datasheet or governing standard.

As a chemistry anchor from the verified composition tables, Inconel 718 spans Ni 50.0-55.0%, Cr 17.0-21.0%, Mo 2.80-3.30% and Nb 4.75-5.50%, and Hastelloy C-276 spans Mo 15.0-17.0%, Cr 14.5-16.5%, Fe 4.0-7.0% and W 3.0-4.5%.

What the standard covers

The grade is chosen on economics as much as temperature: Incoloy 800’s high iron content lowers alloy cost against the Inconel line while keeping good creep-rupture strength and ASME code approval. Its stocked forms run from forging and flange stock through bar and rod, plate and sheet, strip and pipe and tube, B408 owns the rod-and-bar end that machining consumes. For pressure-vessel creep duty above 600 °C the controlled-carbon variants 800H and 800HT take over, but for furnace hardware and general process piping at the 1100 °C ceiling, base-grade 800 bar under B408 is the specification of record.

Grades under this standard

ItemVerified detail
AlloyIncoloy 800 (UNS N08800, GB NS111)
Density7.94 g/cm³
Max service temperature1100 °C
Product form under B408Rod and bar
Companion standardsB163 / B407 (tube), ASME SB-407
Key dutyEthylene furnace tubes, heat exchangers, process piping

How to order against it

Order B408 by UNS, size and condition, hot rolled, forged, cold drawn, peeled or ground are the bar states stocked. Where the part feeds an ASME code job, cite ASME SB-407 for the pressure boundary and B408 for the machined hardware. EN 10204 3.1 heat chemistry is the acceptance basis, matched to the N08800 band.

How to select the right option for your process

Five checks, in order. Each one keeps the component inside its specification:

  1. Step 1: Confirm the maximum service temperature. Fix the peak continuous service temperature the component will see. It decides whether a precipitation-hardened grade such as Inconel 718 (rated 650 °C) or an oxidation-resistant solid-solution grade such as Hastelloy X (rated 1100 °C) is even in the running.
  2. Step 2: Match the environment and alloy family. Identify the corroding or oxidizing media (chlorides, acids, seawater, combustion gas) and match the family: Ni-Cr-Mo for wet corrosion, Ni-Cu for seawater and hydrofluoric acid, cobalt-base for wear and biocompatibility, precision grades for controlled physical properties.
  3. Step 3: Choose the product form. Select the semi-finished form: bar and rod (Ø6-350 mm), plate and sheet (0.5-80 mm), strip (0.05-3.0 mm), pipe and tube (OD 6-219 mm), wire (Ø0.10-12.0 mm) or a forged ring, disc or shaft from 5 kg to 3,000 kg.
  4. Step 4: Set the dimensions and tolerances. State the finished dimensions, condition (hot rolled, cold drawn, solution annealed, spring temper) and surface finish against the form’s stock range, so the mill certificate matches the drawing.
  5. Step 5: State the standard and certificate. Declare the governing ASTM / AMS / GB/T standard and the certification level: EN 10204 3.1 with heat-specific chemistry, or 3.2 third-party witnessed. The grade is proven by the mill test certificate, not assumed.

Frequently Asked Questions (FAQ)

Which alloy does ASTM B408 cover?

Incoloy 800, UNS N08800 (GB NS111), in rod and bar, the cost-effective Ni-Fe-Cr base grade of the 800 family, oxidation and carburization resistant to 1100 °C.

B408 or B407 for a machined furnace fitting?

B408, rod and bar is what machining consumes. B407 is the seamless pipe-and-tube document for the same alloy, and keep the form-standard pairing explicit on the purchase order.

When does base-grade 800 bar stop being the pick?

When the duty is ASME pressure-vessel creep service above 600 °C, there the controlled-carbon 800H (N08810) with its grain-size requirement takes over, supplied under its own ASME documentation.