ASTM B637 governs precipitation-hardening nickel and cobalt alloy bars and forgings, which makes it the single most-cited bar standard on this site: seven stocked grades trace their bar and forging supply to it. If your drawing says a rotating part, a bolt or a hot-section fastener in bar or forged form, this page maps the grades you can actually call out under it.

A superalloy is an alloy engineered for sustained service at high temperature or in aggressive media, and every figure on this page traces back to a verified datasheet or governing standard.

For reference, the precision-alloy anchors are 4J36 (Invar 36) at a near-zero expansion coefficient of about 1.3 × 10⁻⁶/°C from cryogenic to 230 °C, and 1J22 at the highest saturation induction of any commercial soft magnetic material, 2.4 T.

What the standard covers

The standard’s scope is bar and forgings in the age-hardenable families, exactly the forms rotating and fastener hardware is bought in. The grades the site supplies against B637 split by duty: Inconel 718 (N07718) is the workhorse for discs, rings and fasteners with verified strength to 650 °C, and Inconel X-750 (N07750) carries relaxation resistance for springs and bolting to 700 °C, and the Nimonic ladder steps upward, Nimonic 75 (N06075) for sheet-metal combustion components and fixtures, Nimonic 80A (N07080) for valves and blades to 815 °C, Nimonic 90 (N07090) for blades and springs to 920 °C, Nimonic 901 (N09901) for discs and rings to 750 °C, and Waspaloy (N07001) covers creep-rupture duty to 870 °C.

Grades under this standard

GradeUNSGBDensityMax service temp
Inconel 718N07718n/a8.19 g/cm³650 °C
Inconel X-750N07750GH41458.28 g/cm³700 °C
Nimonic 75N06075GH30308.37 g/cm³1000 °C
Nimonic 80AN07080GH4080A8.19 g/cm³815 °C
Nimonic 90N07090GH40908.18 g/cm³920 °C
Nimonic 901N09901GH29018.2 g/cm³750 °C
WaspaloyN07001GH47388.22 g/cm³870 °C

How to order against it

Ordering against B637 is a certificate exercise: state the grade and UNS, the bar or forged form, the condition (solution-treated plus aged, or as your drawing defines), and require an EN 10204 3.1 mill test certificate proving heat chemistry by OES against the standard’s band. Where rotating quality matters, discs, rings, premium fasteners, Inconel 718 is also supplied against AMS 5662 / 5663, and Waspaloy against AMS 5708/5709, and cite those alongside B637 rather than instead of it.

How to select the right option for your process

Five checks, in order. Each one keeps the component inside its specification:

  1. Step 1: Confirm the maximum service temperature. Fix the peak continuous service temperature the component will see. It decides whether a precipitation-hardened grade such as Inconel 718 (rated 650 °C) or an oxidation-resistant solid-solution grade such as Hastelloy X (rated 1100 °C) is even in the running.
  2. Step 2: Match the environment and alloy family. Identify the corroding or oxidizing media (chlorides, acids, seawater, combustion gas) and match the family: Ni-Cr-Mo for wet corrosion, Ni-Cu for seawater and hydrofluoric acid, cobalt-base for wear and biocompatibility, precision grades for controlled physical properties.
  3. Step 3: Choose the product form. Select the semi-finished form: bar and rod (Ø6-350 mm), plate and sheet (0.5-80 mm), strip (0.05-3.0 mm), pipe and tube (OD 6-219 mm), wire (Ø0.10-12.0 mm) or a forged ring, disc or shaft from 5 kg to 3,000 kg.
  4. Step 4: Set the dimensions and tolerances. State the finished dimensions, condition (hot rolled, cold drawn, solution annealed, spring temper) and surface finish against the form’s stock range, so the mill certificate matches the drawing.
  5. Step 5: State the standard and certificate. Declare the governing ASTM / AMS / GB/T standard and the certification level: EN 10204 3.1 with heat-specific chemistry, or 3.2 third-party witnessed. The grade is proven by the mill test certificate, not assumed.

Frequently Asked Questions (FAQ)

Which grades does this site supply under ASTM B637?

Seven: Inconel 718, Inconel X-750, Nimonic 75, Nimonic 80A, Nimonic 90, Nimonic 901 and Waspaloy, each listed against B637 in its datasheet, each supplied as bar or forgings with heat-traceable certification.

Does ASTM B637 cover plate and sheet?

No, its scope is bar and forgings. Plate, sheet and strip for the same grades are governed by their own specifications, and order the product form against the matching standard and say so on the purchase order.

How does B637 relate to the AMS codes?

B637 is the ASTM material specification, and AMS 5662/5663 (Inconel 718) and AMS 5708/5709 (Waspaloy) are aerospace process specifications layered on top for rotating quality. Cite the AMS alongside B637 when the hardware flies.