What Nickel 200 (N02200) can and cannot do on superalloy standards (astm, ams, gb/t) is fixed by the verified envelope below. Datasheet facts on Nickel 200, and the decision they drive for superalloy standards (astm, ams, gb/t). Nothing else.
Nickel 200 (N02200) is a Pure Nickel grade whose datasheet leans on one documented property: 99.6% minimum nickel.
For reference, the verified chemistry bands include Monel K-500 at Ni 63.0-70.0% and Cu 27.0-33.0%, plus Nickel 200 at 99.6% minimum nickel. The certificates cite the same bands.
What Superalloy Standards (ASTM, AMS, GB/T) means for Nickel 200
Start from the verified triple for Nickel 200: 8.89 g/cm³ density, 315 °C ceiling. On superalloy standards (astm, ams, gb/t) the duty decides, and the duty is caustic soda evaporator tubes, spinnerets and electrical terminals.
| Property | Nickel 200 |
|---|---|
| Grade | Nickel 200 (N02200) · GB N6 |
| Density | 8.89 g/cm³ |
| Max service temp | 315 °C |
| Best duty | Caustic soda evaporator tubes, spinnerets and electrical terminals |
| Available forms | Forging, Wire, Flange, Bar & Rod, Plate & Sheet, Strip, Pipe & Tube |
| Standards | ASTM B160, ASTM B161, ASTM B162, ASME SB-160 |
Specification signals
Calling out ASTM B160, ASTM B161, ASTM B162, ASME SB-160 alongside GB N6 is how a drawing tells the mill exactly what Nickel 200 has to meet. In practice the applications list confirms the fit: Nickel 200 is specified for caustic soda evaporator tubes and synthetic fiber spinnerets, not as a universal filler.
- One Nickel 200 datasheet callout does most of the work on this page: Food-grade qualified. A purchasing audit on the Nickel 200 order checks that line first.
In practice
Each standard defines the chemistry band, the mechanical requirements and the test method. The certificate must cite the exact designation on your purchase order. Every shipment for caustic soda evaporator tubes, spinnerets and electrical terminals cites the same governing documents, which is what keeps multi-batch builds interchangeable.
How to select the right option for your process
Five checks, in order. Each one keeps the component inside its specification:
- Step 1: Confirm the maximum service temperature. Fix the peak continuous service temperature the component will see. It decides whether a precipitation-hardened grade such as Inconel 718 (rated 650 °C) or an oxidation-resistant solid-solution grade such as Hastelloy X (rated 1100 °C) is even in the running.
- Step 2: Match the environment and alloy family. Identify the corroding or oxidizing media (chlorides, acids, seawater, combustion gas) and match the family: Ni-Cr-Mo for wet corrosion, Ni-Cu for seawater and hydrofluoric acid, cobalt-base for wear and biocompatibility, precision grades for controlled physical properties.
- Step 3: Choose the product form. Select the semi-finished form: bar and rod (Ø6-350 mm), plate and sheet (0.5-80 mm), strip (0.05-3.0 mm), pipe and tube (OD 6-219 mm), wire (Ø0.10-12.0 mm) or a forged ring, disc or shaft from 5 kg to 3,000 kg.
- Step 4: Set the dimensions and tolerances. State the finished dimensions, condition (hot rolled, cold drawn, solution annealed, spring temper) and surface finish against the form’s stock range, so the mill certificate matches the drawing.
- Step 5: State the standard and certificate. Declare the governing ASTM / AMS / GB/T standard and the certification level: EN 10204 3.1 with heat-specific chemistry, or 3.2 third-party witnessed. The grade is proven by the mill test certificate, not assumed.
Frequently Asked Questions (FAQ)
How does superalloy standards (astm, ams, gb/t) resolve for Nickel 200?
Name the document, name the grade. Rejecting the wrong document at goods-in is cheap, discovering it after fabrication is not, so the citation is checked first.
What is Nickel 200 best used for?
Nickel 200 is stocked for caustic soda evaporator tubes, spinnerets and electrical terminals; the documented edge is that commercially pure wrought nickel (99.6% min) for caustic alkalis and electrical duty.
What forms is Nickel 200 available in?
Stocked forms: Forging, Wire, Flange, Bar & Rod, Plate & Sheet, Strip, Pipe & Tube.
What standards does Nickel 200 meet?
ASTM B160, ASTM B161, ASTM B162, ASME SB-160 are the standards Nickel 200 is supplied against, each order closed by an EN 10204 3.1 mill test certificate.
When does Nickel 200 stop being the right choice?
Nickel 200 stops being right above 315 °C, or in media its family was not built for.