Superalloy Tensile Strength, Yield and Elongation, applied to Nickel 200 (N02200): verified numbers first, then the reasoning a specifier applies to Nickel 200. A RAS Thermal reference page on superalloy tensile strength, yield and elongation.

Nickel 200 is a commercially pure wrought nickel (99.6% minimum) offering excellent corrosion resistance in caustic alkalis, synthetic fiber production and food processing.

As a chemistry anchor from the verified composition tables, Inconel 718 spans Ni 50.0-55.0%, Cr 17.0-21.0%, Mo 2.80-3.30% and Nb 4.75-5.50%, and Hastelloy C-276 spans Mo 15.0-17.0%, Cr 14.5-16.5%, Fe 4.0-7.0% and W 3.0-4.5%.

What Superalloy Tensile Strength, Yield and Elongation means for Nickel 200

What fixes superalloy tensile strength, yield and elongation for Nickel 200 (N02200) is the verified envelope (8.89 g/cm³, 315 °C) read against caustic soda evaporator tubes, spinnerets and electrical terminals.

PropertyNickel 200
GradeNickel 200 (N02200) · GB N6
Density8.89 g/cm³
Max service temp315 °C
Best dutyCaustic soda evaporator tubes, spinnerets and electrical terminals
Available formsForging, Wire, Flange, Bar & Rod, Plate & Sheet, Strip, Pipe & Tube
StandardsASTM B160, ASTM B161, ASTM B162, ASME SB-160

Specification signals

No single tensile figure is claimed for Nickel 200. The envelope is stated per supply condition in the verified data. In practice the applications list confirms the fit: Nickel 200 is specified for caustic soda evaporator tubes and synthetic fiber spinnerets, not as a universal filler.

  • One Nickel 200 datasheet callout does most of the work on this page: 99.6% minimum nickel. A purchasing audit on the Nickel 200 order checks that line first.

In practice

Demand the condition alongside the values. A tensile number without its state is not evidence. That envelope is what caustic soda evaporator tubes, spinnerets and electrical terminals draws on.

How to select the right option for your process

Work through these checks in order so the component stays inside its specification:

  1. Step 1: Confirm the maximum service temperature. Fix the peak continuous service temperature the component will see. It decides whether a precipitation-hardened grade such as Inconel 718 (rated 650 °C) or an oxidation-resistant solid-solution grade such as Hastelloy X (rated 1100 °C) is even in the running.
  2. Step 2: Match the environment and alloy family. Identify the corroding or oxidizing media (chlorides, acids, seawater, combustion gas) and match the family: Ni-Cr-Mo for wet corrosion, Ni-Cu for seawater and hydrofluoric acid, cobalt-base for wear and biocompatibility, precision grades for controlled physical properties.
  3. Step 3: Choose the product form. Select the semi-finished form: bar and rod (Ø6-350 mm), plate and sheet (0.5-80 mm), strip (0.05-3.0 mm), pipe and tube (OD 6-219 mm), wire (Ø0.10-12.0 mm) or a forged ring, disc or shaft from 5 kg to 3,000 kg.
  4. Step 4: Set the dimensions and tolerances. State the finished dimensions, condition (hot rolled, cold drawn, solution annealed, spring temper) and surface finish against the form’s stock range, so the mill certificate matches the drawing.
  5. Step 5: State the standard and certificate. Declare the governing ASTM / AMS / GB/T standard and the certification level: EN 10204 3.1 with heat-specific chemistry, or 3.2 third-party witnessed. The grade is proven by the mill test certificate, not assumed.

Frequently Asked Questions (FAQ)

How does superalloy tensile strength, yield and elongation resolve for Nickel 200?

Asking for the tensile of Nickel 200 without naming a state is asking half a question. The EN 10204 3.1 route closes the gap: heat-specific chemistry plus the stated condition proves the envelope.

What is Nickel 200 best used for?

Caustic soda evaporator tubes, spinnerets and electrical terminals, which is where this grade’s datasheet numbers are actually verified.

What forms is Nickel 200 available in?

The stocked forms are Forging, Wire, Flange, Bar & Rod, Plate & Sheet, Strip, Pipe & Tube; sizes follow the stock range for the form you pick.

What standards does Nickel 200 meet?

ASTM B160, ASTM B161, ASTM B162, ASME SB-160 are the standards Nickel 200 is supplied against, each order closed by an EN 10204 3.1 mill test certificate.

When does Nickel 200 stop being the right choice?

Nickel 200 stops being right above 315 °C, or in media its family was not built for.