Superalloy Tensile Strength, Yield and Elongation, applied to Nimonic 80A (N07080): verified numbers first, then the reasoning a specifier applies to Nimonic 80A. A RAS Thermal reference page on superalloy tensile strength, yield and elongation.

Nimonic 80A (N07080): Ni-Cr-Ti-Al alloy for exhaust valves, turbine blades and high-temperature springs..

As density anchors from the verified datasheets, Hastelloy X verifies 8.22 g/cm³ with oxidation resistance to 1100 °C, Inconel 625 verifies 8.44 g/cm³ to 980 °C, and L605 is the heaviest stocked grade at 9.13 g/cm³.

What Superalloy Tensile Strength, Yield and Elongation means for Nimonic 80A

What fixes superalloy tensile strength, yield and elongation for Nimonic 80A (N07080) is the verified envelope (8.19 g/cm³, 815 °C) read against exhaust valves, turbine blades and high-temperature springs to 815 °C.

PropertyNimonic 80A
GradeNimonic 80A (N07080) · GB GH4080A
Density8.19 g/cm³
Max service temp815 °C
Best dutyExhaust valves, turbine blades and high-temperature springs to 815 °C
Available formsForging, Wire, Spring Wire, Flange, Bar & Rod, Plate & Sheet
StandardsASTM B637, BS HR 201, AMS 5763, DIN 17742

Specification signals

Specification starts from that feature line, Gamma-prime strengthened, and ends with a certificate that proves the heat actually reached it. In practice the applications list confirms the fit: Nimonic 80A is specified for automotive exhaust valves and marine diesel engine valves, not as a universal filler.

  • The feature that separates Nimonic 80A from its nearest neighbours is specific: Good hot hardness. Hold the Nimonic 80A certificate to proving it, not asserting it.

In practice

Cold-quoted datasheets lose arguments at goods-in. exhaust valves, turbine blades and high-temperature springs to 815 °C assumes the datasheet class and relies on the certificate to prove the heat met it.

How to select the right option for your process

Five checks, in order. Each one keeps the component inside its specification:

  1. Step 1: Confirm the maximum service temperature. Fix the peak continuous service temperature the component will see. It decides whether a precipitation-hardened grade such as Inconel 718 (rated 650 °C) or an oxidation-resistant solid-solution grade such as Hastelloy X (rated 1100 °C) is even in the running.
  2. Step 2: Match the environment and alloy family. Identify the corroding or oxidizing media (chlorides, acids, seawater, combustion gas) and match the family: Ni-Cr-Mo for wet corrosion, Ni-Cu for seawater and hydrofluoric acid, cobalt-base for wear and biocompatibility, precision grades for controlled physical properties.
  3. Step 3: Choose the product form. Select the semi-finished form: bar and rod (Ø6-350 mm), plate and sheet (0.5-80 mm), strip (0.05-3.0 mm), pipe and tube (OD 6-219 mm), wire (Ø0.10-12.0 mm) or a forged ring, disc or shaft from 5 kg to 3,000 kg.
  4. Step 4: Set the dimensions and tolerances. State the finished dimensions, condition (hot rolled, cold drawn, solution annealed, spring temper) and surface finish against the form’s stock range, so the mill certificate matches the drawing.
  5. Step 5: State the standard and certificate. Declare the governing ASTM / AMS / GB/T standard and the certification level: EN 10204 3.1 with heat-specific chemistry, or 3.2 third-party witnessed. The grade is proven by the mill test certificate, not assumed.

Frequently Asked Questions (FAQ)

How does superalloy tensile strength, yield and elongation resolve for Nimonic 80A?

The datasheet makes the promise in one line: Gamma-prime strengthened. OES chemistry pins the grade, the stated condition pins the strength, and both have to land on the same certificate.

What is Nimonic 80A best used for?

Exhaust valves, turbine blades and high-temperature springs to 815 °C, which is where this grade’s datasheet numbers are actually verified.

What forms is Nimonic 80A available in?

Nimonic 80A ships as Forging, Wire, Spring Wire, Flange, Bar & Rod, Plate & Sheet, within the stock range of each form.

What standards does Nimonic 80A meet?

Every Nimonic 80A order cites its governing standard (ASTM B637, BS HR 201, AMS 5763, DIN 17742) and arrives with an EN 10204 3.1 certificate proving the heat.

When does Nimonic 80A stop being the right choice?

Nimonic 80A stops being right above 815 °C, or in media its family was not built for.