Disc-grade strength with the deepest supply chain to 650 °C, or creep-rupture pedigree to 870 °C?

Inconel 718 is a precipitation-hardenable nickel-chromium alloy with outstanding strength, corrosion resistance and fabricability.

Route the decision

  • If the part is a disc, ring, shaft or fastener below 650 °C, take Inconel 718: verified 1275 MPa tensile at 38 HRC, 860 MPa still held at 650 °C, and the widest certification infrastructure of any superalloy (AMS 5662/5663, ASTM B637).
  • If the part sees sustained load between 650 and 870 °C, hot-section discs, rings, high-temperature fasteners, take Waspaloy: verified creep-rupture strength across exactly that band, under AMS 5708/5709 and ASTM B637.
  • If microstructural stability under cyclic thermal loading decides, Waspaloy lists it as a verified feature, the thermal-cycling disc duty, and Inconel 718 is the documented choice below its 650 °C ceiling.
  • If supply-chain depth and price stability matter, Inconel 718 is the volume workhorse of the pair, the oil-and-gas and aerospace standard whose certificates every auditor already knows how to read.
PropertyInconel 718Waspaloy
UNS / GBN07718N07001
Density8.19 g/cm³8.22 g/cm³
Max service temp650 °C870 °C
Governing standardsAMS 5662, AMS 5663, ASTM B637, UNS N07718AMS 5708, AMS 5709, AMS 5544, ASTM B637
Stock formsForging, Wire, Spring Wire, Bar, Plate, StripForging, Wire, Flange, Bar & Rod, Plate & Sheet, Strip

Specification signals

Inconel 718 wins the sub-650 °C strength-and-supply axis: 1035 MPa yield aged, spring wire among its stock forms, cryogenic capability included, and a certification trail no other superalloy matches. Waspaloy wins the 650-870 °C band outright: creep-rupture strength verified across that range is precisely what Inconel 718’s datasheet stops short of, with AMS 5708/5709 covering the disc and ring hardware.

  • Inconel 718: Inconel 718 wins the sub-650 °C strength-and-supply axis: 1035 MPa yield aged, spring wire among its stock forms, cryogenic capability included, and a certification trail no other superalloy matches.
  • Waspaloy: Waspaloy wins the 650-870 °C band outright: creep-rupture strength verified across that range is precisely what Inconel 718’s datasheet stops short of, with AMS 5708/5709 covering the disc and ring hardware.

Switch triggers

Specify Waspaloy when peak metal temperature leaves the 650 °C band and the part still carries load, and specify Inconel 718 when the duty sits below 650 °C, or when cryogenic service, spring-wire forms or supply-chain depth decide.

How to select the right option for your process

Work through these checks in order so the component stays inside its specification:

  1. Step 1: Confirm the maximum service temperature. Fix the peak continuous service temperature the component will see. It decides whether a precipitation-hardened grade such as Inconel 718 (rated 650 °C) or an oxidation-resistant solid-solution grade such as Hastelloy X (rated 1100 °C) is even in the running.
  2. Step 2: Match the environment and alloy family. Identify the corroding or oxidizing media (chlorides, acids, seawater, combustion gas) and match the family: Ni-Cr-Mo for wet corrosion, Ni-Cu for seawater and hydrofluoric acid, cobalt-base for wear and biocompatibility, precision grades for controlled physical properties.
  3. Step 3: Choose the product form. Select the semi-finished form: bar and rod (Ø6-350 mm), plate and sheet (0.5-80 mm), strip (0.05-3.0 mm), pipe and tube (OD 6-219 mm), wire (Ø0.10-12.0 mm) or a forged ring, disc or shaft from 5 kg to 3,000 kg.
  4. Step 4: Set the dimensions and tolerances. State the finished dimensions, condition (hot rolled, cold drawn, solution annealed, spring temper) and surface finish against the form’s stock range, so the mill certificate matches the drawing.
  5. Step 5: State the standard and certificate. Declare the governing ASTM / AMS / GB/T standard and the certification level: EN 10204 3.1 with heat-specific chemistry, or 3.2 third-party witnessed. The grade is proven by the mill test certificate, not assumed.

Frequently Asked Questions (FAQ)

Waspaloy vs Inconel 718 for turbine discs?

By temperature band: discs below 650 °C are Inconel 718 territory with the deepest audit trail, and sustained disc duty from 650 to 870 °C is what Waspaloy’s verified creep-rupture strength exists for.

Which grade is stronger at room temperature?

Effectively the same class, Inconel 718 verifies 1275 MPa tensile at 38 HRC aged, and Waspaloy is a comparable age-hardenable grade. The separation happens at temperature, where Waspaloy holds on to 870 °C.

Can Inconel 718 replace Waspaloy above 650 °C?

Not against its datasheet: the verified ceiling is 650 °C. Between 650 and 870 °C, Waspaloy is the only one of the pair with documented creep-rupture capability.

Do they share certification routes?

Both cite ASTM B637 for bar and forgings, and the AMS layers differ, AMS 5662/5663 for Inconel 718, AMS 5708/5709 for Waspaloy. Cite the pair that matches the hardware.