A superalloy is an alloy engineered for sustained service at high temperature or in aggressive media, and every figure on this page traces back to a verified datasheet or governing standard.
For reference, the verified chemistry bands include Monel K-500 at Ni 63.0-70.0% and Cu 27.0-33.0%, plus Nickel 200 at 99.6% minimum nickel. The certificates cite the same bands.
What this page covers
Medical devices select cobalt grades for a reason: biocompatibility plus fatigue life plus MRI compatibility. At RAS Thermal MP35N is biocompatible per ASTM F562 with ultra-high tensile strength (over 1800 MPa achievable) and non-magnetic behavior. L605 is biocompatible per ASTM F90 with wear and galling resistance.
The verified numbers
Every figure on this page is drawn from our verified superalloy datasheets and the governing standards (ASTM B637/B443/B575/B164/B160, AMS, GB/T 14986). Implants: MP35N · L605. Biocompatible: ASTM F562 · F90. Non-magnetic: MP35N (MRI). Fatigue: excellent (both).
What this means for your selection
Medical devices select cobalt grades for a reason: biocompatibility plus fatigue life plus MRI compatibility. At RAS Thermal MP35N is biocompatible per ASTM F562 with ultra-high tensile strength (over 1800 MPa achievable) and non-magnetic behavior. L605 is biocompatible per ASTM F90 with wear and galling resistance. The table below takes each grade’s temperature ceiling, best duty and available form, and the related pages carry the same verified numbers one level deeper. Decision first, then the data behind it.
How to select the right option for your process
Run the list top to bottom before the enquiry goes out, that is what keeps the part inside its specification:
- Step 1: Confirm the maximum service temperature. Fix the peak continuous service temperature the component will see. It decides whether a precipitation-hardened grade such as Inconel 718 (650 °C) or an oxidation-resistant solid-solution grade such as Hastelloy X (1100 °C) is in the running.
- Step 2: Match the environment and alloy family. Identify the corroding or oxidizing media and match the family: Ni-Cr-Mo for wet corrosion, Ni-Cu for seawater and hydrofluoric acid, cobalt-base for wear and biocompatibility, precision grades for controlled physical properties.
- Step 3: Choose the product form. Select the semi-finished form: bar and rod, plate and sheet, strip, pipe and tube, wire, or a forged ring, disc or shaft, against the machined part and quantity.
- Step 4: Set the dimensions and tolerances. State the finished dimensions, condition (hot rolled, cold drawn, solution annealed, spring temper) and surface finish against the form’s stock range.
- Step 5: State the standard and certificate. Declare the governing ASTM / AMS / GB-T standard and the certification level, EN 10204 3.1 with heat-specific chemistry, or 3.2 third-party witnessed.
How the candidate options compare
- MP35N: 8.43 g/cm³ · 425 °C, and typical use: medical implants, aerospace fasteners and high-performance springs.
- L605: 9.13 g/cm³ · 980 °C, and typical use: aerospace bearing races, wear rings and combustion hardware.
Related resources
Each link below takes one grade or one sub-topic and carries the same verified numbers with it.