A superalloy is an alloy engineered for sustained service at high temperature or in aggressive media, and every figure on this page traces back to a verified datasheet or governing standard.

As density anchors from the verified datasheets, Hastelloy X verifies 8.22 g/cm³ with oxidation resistance to 1100 °C, Inconel 625 verifies 8.44 g/cm³ to 980 °C, and L605 is the heaviest stocked grade at 9.13 g/cm³.

What this page covers

Precision alloys are chosen for a controlled physical property, not bulk strength. At RAS Thermal 4J29 (Kovar, ASTM F15) matches borosilicate glass for hermetic seals, and 4J36 (Invar 36) shows near-zero expansion, and 1J22 (HiperCo 50 equivalent) reaches 2.4 T saturation induction, and 1J50 offers permeability above 30,000, and 3J21 is the elastic-spring grade.

The verified numbers

Every figure on this page is drawn from our verified superalloy datasheets and the governing standards (ASTM B637/B443/B575/B164/B160, AMS, GB/T 14986). Expansion: 4J29 · 4J36. Soft magnetic: 1J22 · 1J50. Elastic: 3J21. Standards: F15 · F1684 · GB-T 14986.

What this means for your selection

Precision alloys are chosen for a controlled physical property, not bulk strength. At RAS Thermal 4J29 (Kovar, ASTM F15) matches borosilicate glass for hermetic seals, and 4J36 (Invar 36) shows near-zero expansion, and 1J22 (HiperCo 50 equivalent) reaches 2.4 T saturation induction, and 1J50 offers permeability above 30,000, and 3J21 is the elastic-spring grade. The table below takes each grade’s temperature ceiling, best duty and available form, and the related pages carry the same verified numbers one level deeper. Decision first, then the data behind it.

How to select the right option for your process

Work through these checks in order so the component stays inside its specification:

  1. Step 1: Confirm the maximum service temperature. Fix the peak continuous service temperature the component will see. It decides whether a precipitation-hardened grade such as Inconel 718 (650 °C) or an oxidation-resistant solid-solution grade such as Hastelloy X (1100 °C) is in the running.
  2. Step 2: Match the environment and alloy family. Identify the corroding or oxidizing media and match the family: Ni-Cr-Mo for wet corrosion, Ni-Cu for seawater and hydrofluoric acid, cobalt-base for wear and biocompatibility, precision grades for controlled physical properties.
  3. Step 3: Choose the product form. Select the semi-finished form: bar and rod, plate and sheet, strip, pipe and tube, wire, or a forged ring, disc or shaft, against the machined part and quantity.
  4. Step 4: Set the dimensions and tolerances. State the finished dimensions, condition (hot rolled, cold drawn, solution annealed, spring temper) and surface finish against the form’s stock range.
  5. Step 5: State the standard and certificate. Declare the governing ASTM / AMS / GB-T standard and the certification level, EN 10204 3.1 with heat-specific chemistry, or 3.2 third-party witnessed.

How the candidate options compare

  • 4J29: 8.17 g/cm³ · 450 °C, and typical use: glass-to-metal and ceramic-to-metal seals in electronic packages.
  • 4J36: 8.1 g/cm³ · 230 °C, and typical use: optical benches, LNG tank membranes and cryogenic transfer lines.
  • 1J22: 8.2 g/cm³ · 450 °C, and typical use: solenoid armatures, pole pieces and weight-critical magnetic hardware.
  • 1J50: 8.2 g/cm³ · 450 °C, and typical use: instrument transformer cores, relay armatures and shielding.
  • 3J21: 8.3 g/cm³ · 350 °C, and typical use: precision instrument hairsprings, pressure sensor diaphragms and elastic sensing elements.

The pages below drill into this topic and document the same verified numbers.