A superalloy is an alloy engineered for sustained service at high temperature or in aggressive media, and every figure on this page traces back to a verified datasheet or governing standard.
For reference, the precision-alloy anchors are 4J36 (Invar 36) at a near-zero expansion coefficient of about 1.3 × 10⁻⁶/°C from cryogenic to 230 °C, and 1J22 at the highest saturation induction of any commercial soft magnetic material, 2.4 T.
What this page covers
Controlled thermal expansion is a precision-alloy property, not a superalloy afterthought. At RAS Thermal the expansion line has two verified members: 4J29 (Kovar, ASTM F15), whose expansion coefficient matches borosilicate glass and alumina ceramics for hermetic seals leak-tight to 10⁻⁹ cc He/s, and 4J36 (Invar 36, ASTM F1684), whose near-zero expansion (about 1.3 × 10⁻⁶/°C from cryogenic temperatures to 230 °C) is the dimensional-stability champion behind optical benches, LNG tank membranes and composite tooling.
The verified numbers
Every figure on this page is drawn from our verified superalloy datasheets and the governing standards (ASTM B637/B443/B575/B164/B160, AMS, GB/T 14986). Sealing pick: 4J29 (Kovar) · ASTM F15 · matches borosilicate glass. Stability pick: 4J36 (Invar 36) · α ≈ 1.3 × 10⁻⁶/°C. 4J36 range: cryogenic to 230 °C. Seal leak-tightness: 10⁻⁹ cc He/s (4J29).
What this means for your selection
Controlled thermal expansion is a precision-alloy property, not a superalloy afterthought. At RAS Thermal the expansion line has two verified members: 4J29 (Kovar, ASTM F15), whose expansion coefficient matches borosilicate glass and alumina ceramics for hermetic seals leak-tight to 10⁻⁹ cc He/s, and 4J36 (Invar 36, ASTM F1684), whose near-zero expansion (about 1.3 × 10⁻⁶/°C from cryogenic temperatures to 230 °C) is the dimensional-stability champion behind optical benches, LNG tank membranes and composite tooling. The table below takes each grade’s temperature ceiling, best duty and available form, and the related pages carry the same verified numbers one level deeper. Decision first, then the data behind it.
How to select the right option for your process
Five checks, in order. Each one keeps the component inside its specification:
- Step 1: Confirm the maximum service temperature. Fix the peak continuous service temperature the component will see. It decides whether a precipitation-hardened grade such as Inconel 718 (650 °C) or an oxidation-resistant solid-solution grade such as Hastelloy X (1100 °C) is in the running.
- Step 2: Match the environment and alloy family. Identify the corroding or oxidizing media and match the family: Ni-Cr-Mo for wet corrosion, Ni-Cu for seawater and hydrofluoric acid, cobalt-base for wear and biocompatibility, precision grades for controlled physical properties.
- Step 3: Choose the product form. Select the semi-finished form: bar and rod, plate and sheet, strip, pipe and tube, wire, or a forged ring, disc or shaft, against the machined part and quantity.
- Step 4: Set the dimensions and tolerances. State the finished dimensions, condition (hot rolled, cold drawn, solution annealed, spring temper) and surface finish against the form’s stock range.
- Step 5: State the standard and certificate. Declare the governing ASTM / AMS / GB-T standard and the certification level, EN 10204 3.1 with heat-specific chemistry, or 3.2 third-party witnessed.
How the candidate options compare
- 4J29: 8.17 g/cm³ · 450 °C, and typical use: glass-to-metal and ceramic-to-metal seals in electronic packages.
- 4J36: 8.1 g/cm³ · 230 °C, and typical use: optical benches, LNG tank membranes and cryogenic transfer lines.