A superalloy is an alloy engineered for sustained service at high temperature or in aggressive media, and every figure on this page traces back to a verified datasheet or governing standard.
As a chemistry anchor from the verified composition tables, Inconel 718 spans Ni 50.0-55.0%, Cr 17.0-21.0%, Mo 2.80-3.30% and Nb 4.75-5.50%, and Hastelloy C-276 spans Mo 15.0-17.0%, Cr 14.5-16.5%, Fe 4.0-7.0% and W 3.0-4.5%.
What this page covers
Weldability is a per-grade property. At RAS Thermal Hastelloy C-276 offers good weldability without post-weld heat treatment. Inconel 625 is known for excellent weldability, precipitation-hardened grades like Inconel 718 weld with controlled procedures. The weld filler and procedure follow the grade’s own guidance.
The verified numbers
Every figure on this page is drawn from our verified superalloy datasheets and the governing standards (ASTM B637/B443/B575/B164/B160, AMS, GB/T 14986). No PWHT needed: C-276 · 625. Controlled procedure: 718 (aged). Filler: per-grade. Backing: certified heat.
What this means for your selection
Weldability is a per-grade property. At RAS Thermal Hastelloy C-276 offers good weldability without post-weld heat treatment. Inconel 625 is known for excellent weldability, precipitation-hardened grades like Inconel 718 weld with controlled procedures. The weld filler and procedure follow the grade’s own guidance. The table below takes each grade’s temperature ceiling, best duty and available form, and the related pages carry the same verified numbers one level deeper. Decision first, then the data behind it.
How to select the right option for your process
Five checks, in order. Each one keeps the component inside its specification:
- Step 1: Confirm the maximum service temperature. Fix the peak continuous service temperature the component will see. It decides whether a precipitation-hardened grade such as Inconel 718 (650 °C) or an oxidation-resistant solid-solution grade such as Hastelloy X (1100 °C) is in the running.
- Step 2: Match the environment and alloy family. Identify the corroding or oxidizing media and match the family: Ni-Cr-Mo for wet corrosion, Ni-Cu for seawater and hydrofluoric acid, cobalt-base for wear and biocompatibility, precision grades for controlled physical properties.
- Step 3: Choose the product form. Select the semi-finished form: bar and rod, plate and sheet, strip, pipe and tube, wire, or a forged ring, disc or shaft, against the machined part and quantity.
- Step 4: Set the dimensions and tolerances. State the finished dimensions, condition (hot rolled, cold drawn, solution annealed, spring temper) and surface finish against the form’s stock range.
- Step 5: State the standard and certificate. Declare the governing ASTM / AMS / GB-T standard and the certification level, EN 10204 3.1 with heat-specific chemistry, or 3.2 third-party witnessed.
How the candidate options compare
- Inconel 718: 8.19 g/cm³ · 650 °C, and typical use: rotating hardware, high-strength fasteners and subsea wellhead components from cryogenic to 650 °C.
- Inconel 625: 8.44 g/cm³ · 980 °C, and typical use: seawater piping, chemical processing and subsea connectors where weldability and corrosion resistance decide.
- Hastelloy C-276: 8.89 g/cm³ · 400 °C, and typical use: chemical reactor internals, FGD scrubbers and sour-gas piping where pitting and stress-corrosion cracking are the enemy.
- Hastelloy X: 8.22 g/cm³ · 1100 °C, and typical use: gas turbine combustion chambers, afterburners and furnace hardware above 1000 °C.
- Monel 400: 8.8 g/cm³ · 540 °C, and typical use: seawater piping, HF acid alkylation units and marine shafts.
- Nimonic 80A: 8.19 g/cm³ · 815 °C, and typical use: exhaust valves, turbine blades and high-temperature springs to 815 °C.
- Waspaloy: 8.22 g/cm³ · 870 °C, and typical use: turbine discs, rings, shafts and high-temperature fasteners.
- Nickel 200: 8.89 g/cm³ · 315 °C, and typical use: caustic soda evaporator tubes, spinnerets and electrical terminals.
- MP35N: 8.43 g/cm³ · 425 °C, and typical use: medical implants, aerospace fasteners and high-performance springs.
- L605: 9.13 g/cm³ · 980 °C, and typical use: aerospace bearing races, wear rings and combustion hardware.
- 4J29: 8.17 g/cm³ · 450 °C, and typical use: glass-to-metal and ceramic-to-metal seals in electronic packages.
- 4J36: 8.1 g/cm³ · 230 °C, and typical use: optical benches, LNG tank membranes and cryogenic transfer lines.
- 1J22: 8.2 g/cm³ · 450 °C, and typical use: solenoid armatures, pole pieces and weight-critical magnetic hardware.
- 1J50: 8.2 g/cm³ · 450 °C, and typical use: instrument transformer cores, relay armatures and shielding.
- Incoloy 800: 7.94 g/cm³ · 1100 °C, and typical use: petrochemical furnace tubes, heat exchanger bundles and process piping from 600 to 1100 °C.
- Incoloy 800H: 7.94 g/cm³ · 1100 °C, and typical use: ASME pressure vessels, steam methane reformers and power plant superheaters.
- Incoloy 800HT: 7.94 g/cm³ · 1100 °C, and typical use: hot-formed pressure vessel heads, tube sheets and reformer tubes.
- Incoloy 825: 8.14 g/cm³ · 540 °C, and typical use: sulfuric acid coolers, phosphoric acid evaporators and offshore production piping.
- Incoloy 925: 8.14 g/cm³ · 650 °C, and typical use: sour gas wellhead components, downhole completion tools and high-strength fasteners.
- 3J21: 8.3 g/cm³ · 350 °C, and typical use: precision instrument hairsprings, pressure sensor diaphragms and elastic sensing elements.
Related resources
Follow the links for the per-grade pages, the figures there match the ones on this page.
- weldability, Inconel 718
- weldability, Inconel 625
- weldability, Hastelloy C-276
- weldability, Hastelloy X
- weldability, Monel 400
- weldability, Nimonic 80A
- weldability, Waspaloy
- weldability, Nickel 200
- weldability, MP35N
- weldability, L605
- weldability, 4J29
- weldability, 4J36
- weldability, 1J22
- weldability, 1J50
- weldability, Incoloy 800
- weldability, Incoloy 800H
- weldability, Incoloy 800HT
- weldability, Incoloy 825
- weldability, Incoloy 925
- weldability, 3J21