Inconel 625 Price
What sits behind the price of one kilogram in 2026, which six variables move the number, and how to compare two quotes that were never written on the same basis.
The short answer
§01, SummaryPublished price
No fixed band — priced per enquiry
The metal moves with the nickel index weekly, and the answer depends on form, size, melting route and test scope. A number printed here would be wrong before the next shipment.
Nickel floor today
USD 8.88/kg
58% nickel × LME cash of USD 15,310/t on 2026-11-20. This is the nickel content only — before Cr, Mo, Nb, melting and rolling.
What changes it most
Form → size → melting route → test scope
Two quotes for the same tonnage can differ by 40% without either being wrong, if one is ESR plate and the other is VAR bar with 100% UT.
Cost position by product form
§02, Where each form sitsWe do not publish per-kilogram bands: the alloy charge re-prices with nickel and molybdenum, so any figure here would be out of date before it shipped. What does not change is the relative position of each form — that is what decides which enquiry costs more, and it stays true whatever the index does.
| Product form | Standard | Cost position | Why it sits there |
|---|---|---|---|
| Hot-rolled plate, 3–25 mm | ASTM B443 | Lowest | Standard mill route; the shortest conversion path from melt to product |
| Hot-rolled round bar, 20–60 mm | ASTM B446 | Low to mid | Catalogue sizes are routine; peeling and straightening add steps |
| Cold-rolled sheet, 0.5–3 mm | ASTM B443 | Mid | Cold reduction, annealing and pickling passes, plus finish control |
| Forged bar, 60–200 mm | ASTM B446 | Mid to high | Press capacity, press time and a higher inspection burden |
| Seamless pipe | ASTM B444 | Highest | Piercing and cold drawing; the longest and least forgiving route |
Read it as a ranking, not as a price list. Two enquiries for the same form can still differ by a third — see the six variables in section 04 — but plate will not overtake pipe because nickel moved.
How one kilogram is priced
§03, Cost build-up625 is not priced by the tonne like rebar. It is priced from chemistry upward, then loaded with conversion cost. Every element below is quoted to a range in ASTM B443/B444/B446, so the alloy charge is computed against the certified heat analysis, not against a nominal figure.
| Element | wt % | Role in the cost |
|---|---|---|
| Nickel | 58.0 min | Dominant line; indexed to LME |
| Chromium | 20.0–23.0 | Ferrochrome, moderate volatility |
| Molybdenum | 8.0–10.0 | Second-largest; wide swings |
| Niobium + Tantalum | 3.15–4.15 | Small mass, high unit cost |
| Iron | 5.0 max | Residual; negligible |
Composition basis: ASTM B443 / B444 / B446 (UNS N06625). GB/T equivalent: GH3625.
Worked example — the nickel line
- LME nickel cash, 2026-11-20
- USD 15,310/t
- Per kilogram of nickel
- USD 15.31
- Nickel in 1 kg of 625 (58%)
- USD 8.88
- Sensitivity
- USD 0.58 per USD 1,000/t
Add chromium, molybdenum, niobium and tantalum, then melting, rolling or forging, heat treatment, testing and yield loss. The finished band in section 02 is what that stack looks like after a mill has done it a few thousand times.
Source: LME official cash settlement via Westmetall. Verify the current figure.
Six things that move the number
§04, VariablesProduct form
Plate and bar come off standard mill routes. Seamless pipe needs piercing and cold drawing, which is why the same alloy charges roughly double per kilogram.
Size and tolerance
A commercial-tolerance 40 mm bar is a catalogue item. A 0.1 mm concentricity ring is a forging plus machining job, and machining hours are not alloy-priced.
Melting route
Air-melted or ESR material to ASTM covers most chemical duty. VAR under AMS 5666 for aerospace and nuclear adds conversion cost and a longer route.
Order quantity
A single heat has a minimum economic size. Small lots carry part of that heat's fixed cost, which is why 200 kg can cost more per kilogram than 2 tonnes.
Test scope
Chemistry plus tensile is standard. Add ultrasonic inspection, hardness verification for NACE MR0175, or a third-party witness and you have added days and cost, not a discount.
Documentation level
An EN 10204 3.1 certificate tied to the heat number is normal for this alloy. If a quote does not state the certificate type, that is the first thing to ask about, not the last.
Normalise before you compare
§05, Comparing quotesMost "625 is cheaper here" conclusions are an artefact of two quotes written on different bases. Put both on the same row before you decide.
| Item to normalise | What to ask | Why it changes the number |
|---|---|---|
| Incoterm | FOB, CIF or DAP? | Freight and insurance either are or are not in the figure |
| Melting route | Air / ESR / VAR? | Cleanliness and conversion cost differ materially |
| Certificate | EN 10204 3.1 to the heat? | Traceability paperwork has a real cost |
| Tolerance | Commercial or drawing? | Machining and scrap are charged at alloy price |
| Test scope | UT, PMI, hardness, third party? | Each adds a step and a schedule slot |
| Validity | How long is the price held? | Nominal alloy prices move weekly; a long window is a risk loaded elsewhere |
625 against the grades it competes with
§06, AlternativesUnit cost is shown as a multiple of 316L rather than in dollars, because that ratio holds across markets and currencies better than any single figure.
| Grade | UNS | Cost vs 316L | Max temp | Seawater | Choose it when |
|---|---|---|---|---|---|
| 316L | S31603 | 1× | 400 °C | No | No chlorides, low temperature, budget-first |
| Incoloy 825 | N08825 | 1.5–2× | 540 °C | Limited | Sulphuric/phosphoric acid, moderate chlorides |
| Inconel 625 | N06625 | 3–4× | 980 °C | Yes | Seawater + high temperature + welds without PWHT |
| Hastelloy C-276 | N10276 | 4–6× | 1040 °C | Yes | Wet chlorine, hypochlorite, severe reducing acids |
| Inconel 718 | N07718 | 4–5× | 650 °C (aged) | Limited | Strength at temperature matters more than corrosion |
When 625 is over-specified
§07, Honest adviceBelow 400 °C, no chlorides
316L or 304L does the job at roughly a quarter of the metal cost. We will say so rather than quote you 625.
Sulphuric or phosphoric acid, moderate temperature
Incoloy 825 is usually adequate and materially cheaper. 625 becomes the right answer once chlorides enter the duty.
Strength, not corrosion, is the driver
If you need strength to 650 °C with aging, 718 is the better route. If you need to 980 °C without PWHT, that is exactly where 625 earns the premium.
Six ways buyers overpay
§08, Buying mistakesSpecifying VAR by default. VAR is for aerospace and nuclear. On chemical plant it buys certification you may not need.
Buying to drawing when a mill form would do. A 200 mm bar cut from a forged bloom often replaces a bespoke forging at half the process cost.
Splitting a heat across two suppliers. Two small lots each carry a heat's fixed cost; one consolidated lot usually costs less in total.
Not stating the certificate level. EN 10204 3.1 to the heat is the norm for 625. Discovering that after delivery costs more than specifying it up front.
Comparing a CIF price with an FOB price. Normalise the Incoterm before concluding anything about the metal cost.
Ignoring niobium in the chemistry check. Nb+Ta is 3.15–4.15%. Material at the bottom of that range is cheaper to make and weaker in service; check the certified analysis.
What to send for a firm quote
§09, EnquirySend these seven items and the first reply can be a price rather than a question.
Product form — plate, sheet, bar, forging, wire, flange or pipe
Size, or a drawing if the part is not a mill form
Quantity with unit — pieces, kilograms or metres
Governing standard — ASTM B443 / B444 / B446, AMS 5666 or GB/T GH3625
Test scope and certificate level — EN 10204 3.1, UT, PMI, NACE MR0175
Incoterm and destination port
Required date, and whether partial shipments are acceptable
Lead time, packing and documents
§10, DeliveryLead time
Depends on whether the item is cut from stock or rolled to order, and on the test scope. It is stated as a dated commitment on the quotation, not as a generic promise.
Packing
Bar and plate ship on timber, interleaved and edge-protected; wire ships on spools or in coils. Sea-worthy export packing is confirmed per order against the route.
Documents
Mill test certificate to EN 10204 3.1 with heat number, packing list, invoice, and certificate of origin where the destination requires it. Third-party inspection can be arranged.
Ten questions buyers ask before ordering
§11, Procurement questionsThese are the questions that come up in almost every 625 enquiry. The answers are the same ones our sales engineers give on the phone.
How much does Inconel 625 cost per kg?
We quote per enquiry rather than publishing a band, because the alloy charge moves with nickel and molybdenum and any printed figure would age badly. What can be stated precisely is the metal floor: at 58% nickel and an LME cash price of USD 15,310/t on 2026-11-20, the nickel content of one kilogram of 625 is about USD 8.88 — before chromium, molybdenum, niobium, melting, rolling and testing. Everything above that floor depends on form, size, melting route, test scope and quantity. Send those and you get a number valid for a stated period.
Why is the price of Inconel 625 so much higher than stainless steel?
Because of what is in it. 625 contains 58% minimum nickel, 20–23% chromium, 8–10% molybdenum and 3.15–4.15% niobium plus tantalum. Nickel and molybdenum are the two largest cost lines, and both are exchange-traded commodities. A 316L heats with roughly 10–12% nickel and 2–3% molybdenum, so the raw-material base alone is several times lower.
Does Inconel 625 price change with the LME nickel price?
Yes, and the relationship is direct. Every USD 1,000/t move on LME nickel shifts the nickel content of one kilogram of 625 by about USD 0.58. Molybdenum, niobium and chromium move independently, so the total can diverge from nickel alone. That is why suppliers quote with a validity window rather than a fixed catalogue price.
What is the difference between an FOB price and a landed cost?
FOB covers the material loaded at the Chinese port. Landed cost adds ocean or air freight, insurance, import duty in your country, port and clearance charges, and any third-party inspection you require. On heavy alloy shipments freight is a small share; on small parcels it can dominate. Always compare quotes on the same Incoterm and the same test scope.
Is a cheaper Inconel 625 quote safe to accept?
Only after you normalise what is included. A quote can be lower because the heat is ESR rather than VAR, because the material is off-spec on niobium, because the mill test certificate is a copy rather than an original to EN 10204 3.1, because tolerances are commercial rather than precision, or because the validity window is unrealistically long. Compare chemistry against ASTM B443/B444/B446 and ask which melting route was used.
What does VAR versus ESR do to the price?
Vacuum arc remelting and electroslag remelting both improve cleanliness and homogeneity over air melting, but VAR carries a higher conversion cost and is normally specified for aerospace and nuclear duty under AMS 5666. If your application is chemical or marine rather than flight-critical, ESR or air-melted material to ASTM may be sufficient and materially cheaper. Decide the melting route before you compare prices.
How much does the size and tolerance of the part affect the price?
Significantly. A 20–60 mm hot-rolled bar is a standard mill product; a 300 mm forged ring with 0.1 mm concentricity is a bespoke forging with machining, extra ultrasonic testing and higher scrap. As a rule, the further the item moves from a catalogue mill form towards a finished machined component, the more the price is driven by process hours rather than by metal content.
What should I send to get an accurate Inconel 625 quote?
Product form, size or drawing, quantity with unit (pieces, kg or metres), the governing standard (ASTM B443, B444, B446 or AMS 5666), required test scope and certificate level, delivery Incoterm and destination port, and any NACE MR0175 or third-party inspection requirement. With those six items a mill can price without a second round of questions.
Can Inconel 625 be supplied to NACE MR0175 for sour service?
Yes. 625 is listed for sour service under NACE MR0175 / ISO 15156, subject to the hardness and heat-treatment conditions in the standard. State the requirement on the enquiry, because it adds hardness verification and documentation that are not part of a standard ASTM B446 order.
Is Inconel 625 ever the wrong choice on cost grounds?
Frequently. If the service is below roughly 400 °C with no chlorides, 316L or 304L will do the same job at a quarter of the metal cost. If the duty is sulphuric or phosphoric acid at moderate temperature, Incoloy 825 is usually adequate. 625 earns its premium where seawater, chlorides and temperatures up to 980 °C coincide, or where the part must be welded in place without post-weld heat treatment.
Where to go next
§12, RelatedGrade page
Inconel 625 — full datasheet
Chemistry, mechanical properties and standards in one table set.
Directory
All 37 nickel alloy grades
Compare 625 against the rest of the Inconel, Hastelloy, Incoloy and Monel families.
Forms
Forging, wire, bar and flange
The four forms we make in-house, and the size envelope for each.
Put your own numbers against this page
Send form, size, quantity and standard, and you get a priced reply with the melting route, certificate level and validity window stated — so it can be compared with any other quote on the same basis.
Request an Inconel 625 quote