1J22 alloy products
Material Family / Precision

1J22

HiperCo 50 equivalent: the Fe-Co-V alloy with the highest saturation induction of any soft magnetic material.

Introduction

§01, General

Need maximum flux in minimum volume? 1J22 (HiperCo 50 equivalent) hits 2.4 T saturation induction, the highest of any commercial soft magnetic material. That's why solenoid armatures, pole pieces and magnetic bearing components in aerospace and defense keep specifying an iron-cobalt-vanadium alloy that carries more flux per gram than anything else on the shelf.

GB/T 14986AMS 7717 equivalentASTM A801

Quick Facts

Density
8.2 g/cm³
Max Service Temp
450°C
Series
Precision

Chemical Composition

GB/T 15018, 1J22 (Fe-Co-V), nominal wt%

Element Symbol Content (wt%) Role
Cobalt Co 48.0 – 51.0 High saturation magnetization
Vanadium V 1.4 – 1.8 Ductility & aging control
Carbon C 0.04 max Controlled residual
Iron Fe Balance Base

Mechanical & Physical Properties

Manufacturer datasheet, typical (soft magnetic alloy — mechanicals vary with heat treat)

Property Value Condition
Tensile Strength (annealed) ≈500–700 MPa Typical, annealed
Saturation Flux Density ≈2.35 T Key design property
Curie Temperature ≈940 °C Physical
Density 8.2 g/cm³ Physical

Applicable Standards & Product Forms

1J22 · UNS — · GB/T 1J22

Standard Product Form
GB/T 15018 Cold-rolled strip / bar
WireStripBar & RodForging

Available Product Forms

§02, Forms
WireStripPlate & SheetBar & Rod

Key Characteristics

§03, Features
Highest saturation induction (2.4 T)
HiperCo 50 equivalent
Aerospace solenoid standard
High Curie temperature (940°C)
Weight-critical magnetic applications

Typical Uses

§04, Applications
Aerospace solenoid armatures
Magnetic bearing pole pieces
High-flux generator rotors
Aircraft power generation
Precision electromagnetic actuators

Pricing

How 1J22 is priced

We do not publish a per-kilogram band. The alloy charge re-prices with nickel and molybdenum, and the rest of the number depends on form, size, melting route and test scope — a figure printed here would be stale before it shipped.

This grade specifies nickel as balance rather than as a minimum, so there is no single published figure to anchor the metal content. The price still builds the same way: the alloy charge at index prices, then melting, rolling or forging, heat treatment, testing and yield loss.

Nickel reference: LME official cash settlement via Westmetall, 2026-11-20. Verify the current figure.

What moves the number

Metal content
Ni · Mo · Nb · Cr, at their index prices
Product form
Plate to seamless pipe is the widest step
Size & tolerance
Process hours, not alloy price
Melting route
Air / ESR / VAR
Test scope
UT, PMI, hardness, third-party witness
Send form & quantity for a price

Frequently Asked Questions

1J22 FAQ

What is 1J22 used for?

1J22 is a Precision alloy used in Aerospace solenoid armatures, Magnetic bearing pole pieces, High-flux generator rotors. It offers Highest saturation induction (2.4 T) and HiperCo 50 equivalent.

What is the chemical composition of 1J22?

1J22 is a controlled-composition Precision alloy supplied to GB/T 14986 and AMS 7717 equivalent. We provide the full mill test certificate with heat-specific chemistry on request.

What forms is 1J22 available in?

1J22 is regularly supplied in Wire, Strip, Plate & Sheet, Bar & Rod. Custom forms and dimensions available on request.

What is the maximum service temperature of 1J22?

1J22 is rated for service up to 450°C. Contact our metallurgy team for specific application recommendations.