GH4099
High-tungsten Ni-based alloy for welded combustion chamber and flame tube assemblies.
Introduction
§01, GeneralTungsten buys solid-solution strength at temperature. GH4099 is a Chinese tungsten-strengthened nickel superalloy with excellent weldability, and it can be welded in the solution-treated condition, which keeps combustion chamber and flame tube assemblies straightforward to fabricate. Density is 8.47 g/cm³, so weight budgets need to know.
Quick Facts
- Density
- 8.47 g/cm³
- Max Service Temp
- 1000°C
- Series
- Waspaloy
Chemical Composition
GB/T 14992, GH4099 (Ni-Cr-Co-W-Mo-Al-Ti), nominal wt% — verify before publish
| Element | Symbol | Content (wt%) | Role |
|---|---|---|---|
| Nickel | Ni | Balance | Base |
| Chromium | Cr | 15.0 – 17.0 | Oxidation resistance |
| Cobalt | Co | 8.0 – 10.0 | Phase stability |
| Tungsten | W | 5.0 – 6.5 | Strengthening |
| Molybdenum | Mo | 3.5 – 5.0 | Strengthening |
| Aluminum | Al | 2.5 – 3.5 | γ′ forming |
| Titanium | Ti | 1.0 – 2.0 | γ′ forming |
| Carbon | C | 0.12 max | Controlled residual |
Mechanical & Physical Properties
GB literature, typical (aged)
| Property | Value | Condition |
|---|---|---|
| Tensile Strength (RT) | ≈1100 MPa | Typical, aged |
| Max Service Temperature | 1000 °C | Combustor/vane duty |
| Density | 8.47 g/cm³ | Physical |
Applicable Standards & Product Forms
GH4099 · UNS — · GB/T GH4099
| Standard | Product Form |
|---|---|
| GB/T 14992 | Sheet / bar / forging |
Available Product Forms
§02, FormsKey Characteristics
§03, FeaturesTypical Uses
§04, ApplicationsExplore Related Alloys
More Waspaloy Grades
Rated 870°C, lower than this grade, also used for aircraft, same Waspaloy series.
Rated 870°C, lower than this grade, also used for aircraft, same Waspaloy series.
Rated 900°C, lower than this grade, also used for combustion, same Waspaloy series.
Rated 1000°C, in the same class as this grade, also used for combustion, same Waspaloy series.
Related Nickel Alloys
Rated 1100°C, higher than this grade, also used for combustion, from the Hastelloy series.
Rated 1000°C, in the same class as this grade, also used for combustion, from the Nimonic series.
Rated 700°C, lower than this grade, also used for aircraft, from the Inconel series.
Pricing
How GH4099 is priced
We do not publish a per-kilogram band. The alloy charge re-prices with nickel and molybdenum, and the rest of the number depends on form, size, melting route and test scope — a figure printed here would be stale before it shipped.
This grade specifies nickel as balance rather than as a minimum, so there is no single published figure to anchor the metal content. The price still builds the same way: the alloy charge at index prices, then melting, rolling or forging, heat treatment, testing and yield loss.
Nickel reference: LME official cash settlement via Westmetall, 2026-11-20. Verify the current figure.
What moves the number
- Metal content
- Ni · Mo · Nb · Cr, at their index prices
- Product form
- Plate to seamless pipe is the widest step
- Size & tolerance
- Process hours, not alloy price
- Melting route
- Air / ESR / VAR
- Test scope
- UT, PMI, hardness, third-party witness
Frequently Asked Questions
GH4099 FAQWhat is GH4099 used for?
GH4099 is a Waspaloy alloy used in Welded combustion chambers, Flame tube assemblies, Gas turbine hot-section weldments. It offers Excellent weldability in solution condition and Tungsten solid-solution strengthened.
What is the chemical composition of GH4099?
GH4099 is a controlled-composition Waspaloy alloy supplied to GB/T 14994. We provide the full mill test certificate with heat-specific chemistry on request.
What forms is GH4099 available in?
GH4099 is regularly supplied in Forging, Wire, Bar & Rod, Plate & Sheet, Strip. Custom forms and dimensions available on request.
What is the maximum service temperature of GH4099?
GH4099 is rated for service up to 1000°C. Contact our metallurgy team for specific application recommendations.
Need GH4099 material?
Request a quote with your specification: grade, form, dimensions and quantity.