Two treatment families, two property sets

Solid-solution grades: Inconel 625, Hastelloy C-276, Hastelloy X, Monel 400, Nickel 200 and the Incoloy 800 base, derive their usable properties from composition and a solution anneal. There is no ageing precipitate to grow, so the thermal route is comparatively simple and the property conversation is about form, environment and temperature. Precipitation-hardened grades: the site’s verified set is Inconel 718, Nimonic 80A, Waspaloy, Incoloy 925, only reach their design properties through a controlled solution-plus-age cycle, because the strength comes from a deliberately precipitated phase. Write the wrong route and the chemistry is right while the properties are wrong: identical composition, different heat treatment, different material.

The chain: forge → solution → age

For a wrought precipitation-hardened part the thermal history is a chain, and each link constrains the next:

  1. Forge / hot-work: carried out in a window that keeps the strengthening phase in solution, finishing too cold raises deformation resistance and risks cracking.
  2. Solution treat: dissolves the phase and carbides and sets the grain size, the grain size chosen here cannot be recovered by ageing.
  3. Stabilise (where specified): precipitates a controlled grain-boundary carbide film that pins the boundaries.
  4. Age: precipitates the fine strengthening phase that carries the strength.

The worked routes are on the process pages: Waspaloy forging temperature and heat treatment, and Nimonic 80A heat treatment.

Why grain size is bought, not just chemistry

Grain size is a certified property on the grades where the duty depends on it. Incoloy 800H is supplied solution annealed to ASTM grain size 5 or coarser: that coarse grain is the creep-strength feature the grade is specified for, and a fine-grained heat is a different material for the duty. The same logic runs through the age-hardened grades: a high-temperature solution treatment with slow cooling grows the grain and buys creep-rupture life, while a lower solution temperature with a fast quench freezes a fine grain and buys yield strength and low-cycle fatigue life. Because the split is decided at solution treatment, it belongs on the drawing.

The treatments you can read off a certificate

A certificate that names only “solution treated and aged” cannot show whether the route was correct. The lines that make it auditable are the actual temperatures and hold times at each step, the cooling medium, and the acceptance test: hardness after ageing (Inconel 718 is verified at 38 HRC), stress-rupture results where the duty is creep-critical, and grain size where the grade is bought for it. The certification methods per grade page sets out the chemistry, mechanical and grain-size evidence line by line, and the RFQ spec writer puts the route on the enquiry.

Specify the route, not the condition

The practical rule: name the service the part must give, creep and stress rupture, or tensile and fatigue, and let that select the route explicitly, then require the recorded times and temperatures on the certificate and qualify the process on coupons taken from the same heat. Where the route is nominal, the acceptance document is still the governing standard: ASTM B637 / B670 for precipitation-hardening bar and flat product, AMS 5662 / 5596 / 5708 / 5709 / 5544 / 5763 where aerospace or rotating quality applies, and BS HR 201 or DIN 17742 for the Nimonic family. Two related hubs go deeper on the choice itself: solid-solution vs precipitation-hardened and cold and hot working.

How to select the right option for your process

Five checks, in order. Each one keeps the component inside its specification:

  1. Step 1: Fix the property the part must hold. Decide whether the component is bought for creep-rupture life, tensile strength and fatigue, or corrosion resistance, because that choice, not the grade name, selects the heat-treatment route.
  2. Step 2: Pick the treatment family. Solid-solution grades (Inconel 625, Hastelloy C-276, Hastelloy X, Monel 400, Nickel 200) get their properties from composition and annealing; precipitation-hardened grades (Inconel 718, Waspaloy, Nimonic 80A, Incoloy 925) need a deliberate solution-plus-age cycle.
  3. Step 3: Write the thermal route on the drawing. State the solution temperature and hold, the cooling medium, the ageing or stabilisation steps and their hold times, not just the condition name. From identical chemistry, different routes give different properties.
  4. Step 4: Set the acceptance test. Name the test that proves the route: hardness after ageing, stress-rupture where the duty is creep-critical, and grain size where the grade is bought for it (Incoloy 800H is supplied at ASTM grain size 5 or coarser).
  5. Step 5: Require the times and temperatures on the certificate. Ask for EN 10204 3.1 with the recorded solution, stabilisation and ageing temperatures and hold times, so the route is auditable rather than asserted.

Follow the links for the per-grade pages, the figures there match the ones on this page.