Room- and elevated-temperature tensile data for the 2 stocked grades with full datasheet tables: Inconel 718 (aged) and Hastelloy C-276 (solution annealed). Grades without a verified table are honestly absent.
| Temperature | UTS | Yield (0.2 %) | Elongation | Hardness |
|---|---|---|---|---|
| Room temperature | 1275 MPa | 1035 MPa | 12% | 38 HRC |
| 540 °C | 1105 MPa | 965 MPa | 14% | , |
| 650 °C | 860 MPa | 795 MPa | 18% | , |
| Temperature | UTS | Yield (0.2 %) | Elongation | Hardness |
|---|---|---|---|---|
| Room temperature | 790 MPa | 355 MPa | 40% | 90 HRB |
| 200 °C | 710 MPa | 320 MPa | 42% | , |
| 400 °C | 620 MPa | 300 MPa | 45% | , |
The remaining stocked grades verify their service behaviour through temperature ceilings, corrosion data and standards rather than a full tensile table, the temperature table covers all grades, and each grade page states exactly what its datasheet documents.
Because the table only carries verified data. A row appears where the grade's page on this site documents a mechanical-properties table in its own right; where no such table exists, the tool says so instead of padding the list with estimated figures. The documented grades here are the two the site verifies in full.
The condition stated on each grade's own datasheet: Inconel 718 in the fully precipitation-hardened condition (solution + double age), Hastelloy C-276 in the solution-annealed condition. The condition line is part of the data, the same alloy in another condition is a different strength envelope.
Each row is the tested floor at that temperature: room temperature, then the elevated-temperature points the datasheet documents. Strength falls as temperature rises; the elongation usually rises with it. Use the row that matches your service temperature, not the room-temperature row.
Send the duty, temperature, stress, media, and we recommend from the full stock range with the certificate data each grade can actually prove.
Send your requirement