Reference table

Weldability by alloy

The verified weldability statement for each of the 20 stocked grades: from Inconel 718's documented weldability to C-276's no-post-weld-heat-treatment route: with the matching AWS A5.14 filler where one is documented, and honest flags where no claim is.

Alloy Verified weldability statement Post-weld heat treatment AWS A5.14 filler Joining notes
Inconel 718N07718 Excellent fabricability and weldability Not documented for this grade. ERNiFeCr-2 ,
Inconel 625N06625 Excellent weldability Not documented for this grade. ERNiCrMo-3 ,
Hastelloy C-276N10276 Good weldability without post-weld heat treatment No post-weld heat treatment required (verified feature). ERNiCrMo-4 ,
Hastelloy XN06002 No weldability claim in the verified feature set, qualify the procedure against the datasheet. Not documented for this grade. ERNiCrMo-2 ,
Monel 400N04400 No weldability claim in the verified feature set, qualify the procedure against the datasheet. Not documented for this grade. ERNiCu-7 ,
Nimonic 80AN07080 No weldability claim in the verified feature set, qualify the procedure against the datasheet. Not documented for this grade. , ,
WaspaloyN07001 No weldability claim in the verified feature set, qualify the procedure against the datasheet. Not documented for this grade. , ,
Nickel 200N02200 No weldability claim in the verified feature set, qualify the procedure against the datasheet. Not documented for this grade. , ,
MP35NR30035 No weldability claim in the verified feature set, qualify the procedure against the datasheet. Not documented for this grade. , ,
L605R30605 No weldability claim in the verified feature set, qualify the procedure against the datasheet. Not documented for this grade. , ,
4J29, No weldability claim in the verified feature set, qualify the procedure against the datasheet. Not documented for this grade. , Good plating and brazing
4J36, No weldability claim in the verified feature set, qualify the procedure against the datasheet. Not documented for this grade. , ,
1J22, No weldability claim in the verified feature set, qualify the procedure against the datasheet. Not documented for this grade. , ,
1J50, No weldability claim in the verified feature set, qualify the procedure against the datasheet. Not documented for this grade. , ,
Incoloy 800N08800 No weldability claim in the verified feature set, qualify the procedure against the datasheet. Not documented for this grade. ERNiCr-3 ,
Incoloy 800HN08810 No weldability claim in the verified feature set, qualify the procedure against the datasheet. Not documented for this grade. , ,
Incoloy 800HTN08811 No weldability claim in the verified feature set, qualify the procedure against the datasheet. Not documented for this grade. , ,
Incoloy 825N08825 No weldability claim in the verified feature set, qualify the procedure against the datasheet. Not documented for this grade. , ,
Incoloy 925N09925 No weldability claim in the verified feature set, qualify the procedure against the datasheet. Not documented for this grade. , ,
3J21, No weldability claim in the verified feature set, qualify the procedure against the datasheet. Not documented for this grade. , ,

Filler selection, post-weld rules and dissimilar-joint logic: welding consumables matching · weldability hub · verified heat-treatment cycles

Frequently Asked Questions (FAQ)

What does an empty weldability row mean?

Exactly what it says: the grade's verified feature set on this site documents no weldability claim. That is not a verdict against welding, it means the weld procedure (filler, preheat, post-weld heat treatment) must be qualified against the grade datasheet before fabrication, rather than assumed from a marketing line.

Why is the post-weld heat treatment question attached to C-276?

Because it is the documented exception: Hastelloy C-276 verifies good weldability without post-weld heat treatment, which is what makes as-welded vessel construction viable in the low-carbon C family.

Does any precision grade have a joining claim?

4J29 verifies good plating and brazing, the joining routes that matter for hermetic glass-to-metal packages, where brazing rather than fusion welding is the process.

Where do the AWS filler classifications come from?

The AWS A5.14 bare-wire classification system, ERNiFeCr-2 for Alloy 718, ERNiCrMo-3 for 625, ERNiCrMo-4 for C-276 and so on. The pairing page carries the full table with the weld-metal behaviour and the post-weld rule each class implies.

Welding into a pressure boundary?

Send the joint design and duty. We reply with the grade, condition and the certificate that proves the heat before and after the weld.

Send your requirement
Request a Quote
Add RAS Thermal as a preferred source on Google