Hastelloy C22
Ni-Cr-Mo-W alloy with superior oxidizing media resistance and better weldability than C-276.
Introduction
§01, GeneralOxidizing media is where C22 pulls ahead of C-276, and it welds more easily too. The Ni-Cr-Mo-W chemistry covers both oxidizing and reducing environments, which suits flue gas desulfurization systems and pharmaceutical processing. When a vessel sees mixed duty, this is the upgrade path.
Cross-Reference
Quick Facts
- UNS
- N06022
- Density
- 8.69 g/cm³
- Max Service Temp
- 600°C
- Series
- Hastelloy
Chemical Composition
ASTM B574 / B575 (N06022), wt%
| Element | Symbol | Content (wt%) | Role |
|---|---|---|---|
| Nickel | Ni | Balance | Base matrix |
| Chromium | Cr | 20.0 – 22.5 | Oxidizing-media resistance |
| Molybdenum | Mo | 12.5 – 14.5 | Reducing-media resistance |
| Iron | Fe | 2.0 – 6.0 | Controlled addition |
| Tungsten | W | 2.5 – 3.5 | Strengthening |
| Vanadium | V | 0.35 max | Controlled residual |
| Cobalt | Co | 2.5 max | Controlled residual |
| Carbon | C | 0.015 max | Grain-boundary carbide control |
Mechanical & Physical Properties
ASTM B574, annealed, room temperature
| Property | Value | Condition |
|---|---|---|
| Tensile Strength | 690 MPa min | Annealed, RT |
| Yield Strength (0.2% offset) | 310 MPa min | Annealed, RT |
| Elongation | 45% min | Annealed, RT |
| Density | 8.69 g/cm³ | Physical |
Applicable Standards & Product Forms
Hastelloy C22 · UNS N06022 · GB/T —
| Standard | Product Form |
|---|---|
| ASTM B574 | Bar |
| ASTM B575 | Plate, Sheet & Strip |
| ASME Section VIII | Pressure vessel code use |
| NACE MR0175 | Sour service compliance |
Available Product Forms
§02, FormsKey Characteristics
§03, FeaturesTypical Uses
§04, ApplicationsExplore Related Alloys
More Hastelloy Grades
Rated 650°C, in the same class as this grade, also used for pharmaceutical, same Hastelloy series.
Rated 650°C, in the same class as this grade, also used for pharmaceutical, same Hastelloy series.
Rated 600°C, in the same class as this grade, also used for processing, same Hastelloy series.
Rated 400°C, lower than this grade, also used for desulfurization, same Hastelloy series.
Related Nickel Alloys
Rated 540°C, lower than this grade, also used for chemical, from the Incoloy series.
Rated 540°C, lower than this grade, also used for processing, from the Monel series.
Rated 980°C, higher than this grade, also used for processing, from the Inconel series.
Pricing
How Hastelloy C22 is priced
We do not publish a per-kilogram band. The alloy charge re-prices with nickel and molybdenum, and the rest of the number depends on form, size, melting route and test scope — a figure printed here would be stale before it shipped.
This grade specifies nickel as balance rather than as a minimum, so there is no single published figure to anchor the metal content. The price still builds the same way: the alloy charge at index prices, then melting, rolling or forging, heat treatment, testing and yield loss.
Nickel reference: LME official cash settlement via Westmetall, 2026-11-20. Verify the current figure.
What moves the number
- Metal content
- Ni · Mo · Nb · Cr, at their index prices
- Product form
- Plate to seamless pipe is the widest step
- Size & tolerance
- Process hours, not alloy price
- Melting route
- Air / ESR / VAR
- Test scope
- UT, PMI, hardness, third-party witness
Frequently Asked Questions
Hastelloy C22 FAQWhat is Hastelloy C22 used for?
Hastelloy C22 is a Hastelloy alloy used in Flue gas desulfurization (FGD) scrubbers, Pharmaceutical processing equipment, Chemical reactor vessels. It offers Superior oxidizing media resistance and Better weldability than C-276.
What is the chemical composition of Hastelloy C22?
Hastelloy C22 is a controlled-composition Hastelloy alloy supplied to ASME Section VIII and ASTM B574. We provide the full mill test certificate with heat-specific chemistry on request.
What forms is Hastelloy C22 available in?
Hastelloy C22 is regularly supplied in Forging, Wire, Flange, Bar & Rod, Plate & Sheet, Pipe & Tube. Custom forms and dimensions available on request.
What is the maximum service temperature of Hastelloy C22?
Hastelloy C22 is rated for service up to 600°C. Contact our metallurgy team for specific application recommendations.
Need Hastelloy C22 material?
Request a quote with your specification: grade, form, dimensions and quantity.