Inconel 718 Plus alloy products
Material Family / Inconel

Inconel 718 Plus

Next-generation Inconel 718 with 50°C higher temperature capability for advanced turbine engines.

Introduction

§01, General

Same fabricability as 718, fifty more degrees. 718 Plus tunes the Al+Ti ratio and balances Nb+Ta to push service temperature from 650°C to 704°C while keeping the workhorse's welding and forming behavior. Next-generation turbine engines get the extra margin without a new supply chain.

Cross-Reference

GB/T: GB GH4169D
Series: Inconel
Density: 8.19 g/cm³
Max Temp: 704°C
Standards: AMS pending · Similar to AMS 5662/5663

Quick Facts

GB
GH4169D
Density
8.19 g/cm³
Max Service Temp
704°C
Series
Inconel

Chemical Composition

ATI 718Plus published nominal, wt% — verify before publish

Element Symbol Content (wt%) Role
Nickel Ni ≈52.5 Base matrix
Chromium Cr ≈18.0 Oxidation resistance
Cobalt Co ≈9.0 Phase stability to 704 °C
Niobium Nb ≈5.45 γ″ strengthening
Molybdenum Mo ≈2.7 Strengthening
Tungsten W ≈1.0 Strengthening
Aluminum Al ≈1.5 γ′ strengthening
Titanium Ti ≈1.0 γ′ strengthening
Iron Fe Balance Base

Mechanical & Physical Properties

Manufacturer datasheet, typical (aged)

Property Value Condition
Tensile Strength (RT) ≈1380 MPa Typical, aged
Max Service Temperature 704 °C vs 650 °C for standard 718
Density 8.19 g/cm³ Physical

Applicable Standards & Product Forms

Inconel 718 Plus · UNS — · GB/T GH4169D

Standard Product Form
AMS pending Aerospace bar & forging (spec in progress)
Similar to AMS 5662/5663 Cross-reference heat treatment
ForgingWireFlangeBar & Rod

Available Product Forms

§02, Forms
ForgingWireFlangeBar & Rod

Key Characteristics

§03, Features
704°C service vs 650°C for 718
Similar fabricability to 718
Optimized gamma-prime/gamma-double-prime
Next-gen turbine qualified
Backward compatible with 718 tooling

Typical Uses

§04, Applications
Advanced gas turbine discs
High-pressure compressor components
Next-gen aero-engine hardware
Oil & gas completion tools

Pricing

How Inconel 718 Plus is priced

We do not publish a per-kilogram band. The alloy charge re-prices with nickel and molybdenum, and the rest of the number depends on form, size, melting route and test scope — a figure printed here would be stale before it shipped.

This grade specifies nickel as balance rather than as a minimum, so there is no single published figure to anchor the metal content. The price still builds the same way: the alloy charge at index prices, then melting, rolling or forging, heat treatment, testing and yield loss.

Nickel reference: LME official cash settlement via Westmetall, 2026-11-20. Verify the current figure.

What moves the number

Metal content
Ni · Mo · Nb · Cr, at their index prices
Product form
Plate to seamless pipe is the widest step
Size & tolerance
Process hours, not alloy price
Melting route
Air / ESR / VAR
Test scope
UT, PMI, hardness, third-party witness
Send form & quantity for a price

Frequently Asked Questions

Inconel 718 Plus FAQ

What is Inconel 718 Plus used for?

Inconel 718 Plus is a Inconel alloy used in Advanced gas turbine discs, High-pressure compressor components, Next-gen aero-engine hardware. It offers 704°C service vs 650°C for 718 and Similar fabricability to 718.

What is the chemical composition of Inconel 718 Plus?

Inconel 718 Plus is a controlled-composition Inconel alloy supplied to AMS pending and Similar to AMS 5662/5663. We provide the full mill test certificate with heat-specific chemistry on request.

What forms is Inconel 718 Plus available in?

Inconel 718 Plus is regularly supplied in Forging, Wire, Flange, Bar & Rod. Custom forms and dimensions available on request.

What is the maximum service temperature of Inconel 718 Plus?

Inconel 718 Plus is rated for service up to 704°C. Contact our metallurgy team for specific application recommendations.

Need Inconel 718 Plus material?

Request a quote with your specification: grade, form, dimensions and quantity.

Request a Quote
Add RAS Thermal as a preferred source on Google