A superalloy is an alloy engineered for sustained service at high temperature or in aggressive media, and every figure on this page traces back to a verified datasheet or governing standard.
As strength anchors from the verified feature sets, MP35N achieves over 1800 MPa tensile while staying non-magnetic per ASTM F562, and Nimonic 80A carries gamma-prime strengthening with service to 815 °C.
What this page covers
Soft magnetic precision alloys are routed by which magnetic property the design actually buys. At RAS Thermal the line has two verified members: 1J22 (HiperCo 50 equivalent), the iron-cobalt-vanadium grade with the highest saturation induction of any commercial soft magnetic material at 2.4 T and a 940 °C Curie temperature, the weight-critical aerospace pick, and 1J50, the 50% Ni-Fe grade whose initial permeability above 30,000 and coercivity below 8 A/m make it the transformer-core and shielding standard.
The verified numbers
Every figure on this page is drawn from our verified superalloy datasheets and the governing standards (ASTM B637/B443/B575/B164/B160, AMS, GB/T 14986). Flux-density pick: 1J22 · 2.4 T saturation · 940 °C Curie. Permeability pick: 1J50 · >30,000 initial · <8 A/m coercivity. Standards: GB-T 14986 · ASTM A801 (1J22) · IEC 60404-8-6 (1J50). 1J50 formability: good cold formability for laminations.
What this means for your selection
Soft magnetic precision alloys are routed by which magnetic property the design actually buys. At RAS Thermal the line has two verified members: 1J22 (HiperCo 50 equivalent), the iron-cobalt-vanadium grade with the highest saturation induction of any commercial soft magnetic material at 2.4 T and a 940 °C Curie temperature, the weight-critical aerospace pick, and 1J50, the 50% Ni-Fe grade whose initial permeability above 30,000 and coercivity below 8 A/m make it the transformer-core and shielding standard. The table below takes each grade’s temperature ceiling, best duty and available form, and the related pages carry the same verified numbers one level deeper. Decision first, then the data behind it.
How to select the right option for your process
Run the list top to bottom before the enquiry goes out, that is what keeps the part inside its specification:
- Step 1: Confirm the maximum service temperature. Fix the peak continuous service temperature the component will see. It decides whether a precipitation-hardened grade such as Inconel 718 (650 °C) or an oxidation-resistant solid-solution grade such as Hastelloy X (1100 °C) is in the running.
- Step 2: Match the environment and alloy family. Identify the corroding or oxidizing media and match the family: Ni-Cr-Mo for wet corrosion, Ni-Cu for seawater and hydrofluoric acid, cobalt-base for wear and biocompatibility, precision grades for controlled physical properties.
- Step 3: Choose the product form. Select the semi-finished form: bar and rod, plate and sheet, strip, pipe and tube, wire, or a forged ring, disc or shaft, against the machined part and quantity.
- Step 4: Set the dimensions and tolerances. State the finished dimensions, condition (hot rolled, cold drawn, solution annealed, spring temper) and surface finish against the form’s stock range.
- Step 5: State the standard and certificate. Declare the governing ASTM / AMS / GB-T standard and the certification level, EN 10204 3.1 with heat-specific chemistry, or 3.2 third-party witnessed.
How the candidate options compare
- 1J22: 8.2 g/cm³ · 450 °C, and typical use: solenoid armatures, pole pieces and weight-critical magnetic hardware.
- 1J50: 8.2 g/cm³ · 450 °C, and typical use: instrument transformer cores, relay armatures and shielding.
Related resources
Follow the links for the per-grade pages, the figures there match the ones on this page.